Alloy Digest (2012) 61 (6): SA-656.
Published: 01 June 2012
... RUUKKI RAEX 450 (typical yield strength 1200 MPa) is part of the Raex family of high-strength and wear-resistant steels with favorable hardness and impact toughness to extend life and decrease wear in structural components. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2012) 61 (7): SA-658.
Published: 01 July 2012
... RUUKKI RAEX 500 (typical yield strength 1250 MPa) is part of the Raex family of high-strength and wear-resistant steels with favorable hardness and impact toughness to extend life and decrease wear in structural components. This datasheet provides information on composition, physical properties...