Alloy Digest (2011) 60 (6): CS-164.
Published: 01 June 2011
... RUUKKI LASER 250C is a structural steel that was developed to be easy to cut, weld, and bend. It is optimized for laser cutting in particular. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness. It also...