... RQT 601 is a quenched and tempered structural steel available in thicknesses 8 to 80 mm (0.3 to 3.0 in.) that combines high strength with excellent forming and welding performance. Originally published as Alloy Digest SA-665, December 2012, revised April 2014. This datasheet provides information...
Journal Articles
Alloy Digest (2012) 61 (10): SA-665.
Published: 01 October 2012
... RQT 601 is a quenched and tempered structural steel available in thicknesses 8 to 80 mm (0.3 to 3.0 in.) that combines high strength with excellent forming and welding performance. Revised as Alloy Digest SA-698, April 2014. This datasheet provides information on composition, physical properties...