Alloy Digest (1976) 25 (1): Ni-223.
Published: 01 January 1976
... Round Permalloy 80 is an 80% nickel-iron-molybdenum alloy that provides very high initial and maximum magnetic permeabilities and minimal core losses at low field strengths. This vacuum-melted product also offers the advantages of small size and weight in magnetic core and shielding materials for...
Journal Articles
Alloy Digest (1982) 31 (12): Fe-68.
Published: 01 December 1982
... METGLAS Alloy 2605S-3 is an amorphous iron-base soft magnetic alloy that can be annealed to obtain a round B-H loop which results in very low core loss at high frequencies (>1kHz). Because of its high saturation induction relative to ferrites or permalloys, significant size reductions are...