Journal Articles
Alloy Digest (1979) 28 (10): Ti-73.
Published: 01 October 1979
... RMI 70 is the highest strength grade of commercially pure unalloyed titanium. It has a guaranteed minimum yield strength of 70,000 psi with good ductility and formability. It has excellent resistance to corrosion by marine atmospheres and seawater. It is used in the aircraft, marine and chemical...
Journal Articles
Alloy Digest (1980) 29 (9): Ti-79.
Published: 01 September 1980
... at room temperature. However, warm forming at 800-1300°F can materially reduce springback and the power required for the operation. Data on cold (70°F) bend radii are given in Table 4. RMI 6AldV-2Sn can be deep drawn to severe depths and spun in the neiahborhood of lOOO-12OOOF in a single operation...
Journal Articles
Alloy Digest (1981) 30 (1): Ti-81.
Published: 01 January 1981
... for the operation. Data on cold (70°F) bend radii are given in Table 3. RMI 55 can be deep drawn to severe depths and spun in the neighborhood of 800°F ln a single operation. Powdered graphite is used as a draw lubricant at this temperature. Multi-stage drawing can be accomplished at room temperature with inter...
Journal Articles
Alloy Digest (1988) 37 (12): Ti-89.
Published: 01 December 1988
... RMI 6A1-4V ELI is an alpha-beta type of titanium-base alloy that can be strengthened by age hardening. In the mill-annealed condition it has a guaranteed minimum room-temperature yield strength of 120,000 psi and can be increased to as much as 160,000 psi by solution treating and aging. This alloy...
Journal Articles
Alloy Digest (1988) 37 (2): Ti-90.
Published: 01 February 1988
... RMI 5A1-2.5Sn is an alpha titanium alloy. It is not hardenable by heat treatment. The relatively high aluminum content gives the alloy good strength characteristics and resistance to elevated-temperature oxidation (up to 1100 F). RMI 5A1-2.5Sn is readily weldable. This datasheet provides...
Journal Articles
Alloy Digest (1987) 36 (9): Ti-88.
Published: 01 September 1987
... RMI 6AI-4V is an alpha-beta type of titanium-base alloy that can be strengthened by age hardening. In the mill-annealed condition it has a guaranteed minimum room-temperature yield strength of 120,000 psi and this can be increased to as much as 160,000 psi by solution treating and aging...
Journal Articles
Alloy Digest (1981) 30 (4): Ti-82.
Published: 01 April 1981
... RMI 8Mn is an alpha-beta titanium alloy that provides a guaranteed room-temperature minimum tensile strength of 120,000 psi in the mill-annealed condition. This alloy offers good formability and excellent resistance to corrosion in applications requiring high strength-to-weight ratios...
Journal Articles
Alloy Digest (1980) 29 (7): Ti-78.
Published: 01 July 1980
... RMI 5A1-5Sn-2Zr-2Mo-Si is an alpha-type titanium alloy recommended for high-temperature applications in the 800-1000 F range. In the mill annealed condition it has a typical room-temperature yield strength of 126,000 psi and a typical yield strength (in short-time elevated-temperature tensile test...
Journal Articles
Alloy Digest (1982) 31 (2): Ti-84.
Published: 01 February 1982
... at 1750-1850°F. Some forming operations on sheet stock can be performed succes&uRy at room temperature. However, warm forming at 800-1400°F can materially reduce springback and the power required for the operation. Data on cold (70°F) bend radii are given in Table 3. Weldability: RMI 8Al-lMo-IV has only...
Journal Articles
Alloy Digest (1979) 28 (8): Ti-72.
Published: 01 August 1979
... RMI 40 is a grade of commercially pure unalloyed titanium. It has a guaranteed minimum yield strength of 40,000 psi with good ductility and formability. Its strength is about the same as that of the annealed austenitic stainless steels. It has good impact properties at low temperatures...
Journal Articles
Alloy Digest (1980) 29 (4): Ti-76.
Published: 01 April 1980
... RMI 25 is a grade of commercially pure titanium. It has a guaranteed minimum yield strength of 25,000 psi with good ductility and formability. Its yield strength is about the same as that of the annealed austenitic stainless steels of lowest yield strength. It has excellent resistance to corrosion...
Journal Articles
Alloy Digest (1979) 28 (12): Ti-74.
Published: 01 December 1979
... RMI 0.2% Pd is a grade of commercially pure titanium to which up to 0.2% palladium has been added. It has a guaranteed minimum yield strength of 40,000 psi with good ductility and formability. It is recommended for corrosion resistance in the chemical industry and other places where...
Journal Articles
Alloy Digest (2001) 50 (8): Ti-117.
Published: 01 August 2001
... as fracture toughness and creep. It also includes information on high temperature performance. Filing Code: TI-117. Producer or source: RMI Company. Producer or Source: RMI Company Copyright © ASM International® 2001 2001 ASM International chemical composition creep strength elasticity...
Journal Articles
Alloy Digest (1981) 30 (8): Ti-83.
Published: 01 August 1981
... temperature. However, warm forming at 800-13OOOF can materially reduce springback and the power required for the operation. Data on cold (70°F) bend radii are given in Tables 3 and 6. Weldability: RMI 6Al-2Sn4Zr-2Mo has only fair weldability but it can be welded successfully under proper conditions...
Journal Articles
Alloy Digest (2021) 70 (6): Ti-179.
Published: 01 June 2021
... (5.6)(b) 16 (9.25)(b) 0.42 0.52 (253 313)(b) RT = room temperature. (a) Source: Titanium Alloy Guide, RMI Titanium Company, Source: Titanium Alloy Guide, RMI Titanium Company, 2000, p 19 2000, p 19. (b) Source: Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Volume 2, ASM...
Journal Articles
Alloy Digest (2004) 53 (7): Ti-134.
Published: 01 July 2004
... in the solution treated condition and its high strength and ductility in the solution treated and aged condition. Allvac is a registered trademark and 38-644 is a trademark of ATI Properties, Inc. Beta C is a trademark of RMI Titanium Company Fig. 1 Thermal conductivity Fig. 2 Elevated-temperature tensile...
Journal Articles
Alloy Digest (1968) 17 (3): Ti-56.
Published: 01 March 1968
... and hydrochloric acids. It can also be used in elevated temperature envimtunents that fluctuate between oxi- dixiag and reducing. Equivalents: A-40 Pd Crucible Steel Company of America HA-194OPd Harvey Aluminum Company RMI-0.2Pd Reactive Metals Company General Characteristics: This alloy is a simple and relatively...
Journal Articles
Alloy Digest (1965) 14 (10): Ti-45.
Published: 01 October 1965
... be used in elevated temperature environments chat fluccuace between oxi- dixiag and reducing. Equivalents: A-40 Pd Crucible Steel Company of America HA-194OPd Harvey Aluminum Company RMI-0.2Pd Reactive Metals Company General Characteristics: This alloy is a simple and relatively inexpensive 0.1% addition...
Journal Articles
Alloy Digest (2021) 70 (2): Ti-175.
Published: 01 February 2021
... Carbon CP Grade 7 Titanium (UNS R52400)(b) Electrical m 0.42 0.52 resistivity circular- (253 313)(c) 0.08 0.08 mil/ft) Oxygen 0.25 0.25 RT = room temperature. (a) Titanium Alloy Guide, RMI Titanium Company, 2000, p.19. (b) Source: Properties and Selection: Nonferrous Alloys and Special-Purpose Materials...
Journal Articles
Alloy Digest (2002) 51 (9): Ti-130.
Published: 01 September 2002
.... A specialized application for this alloy is aircraft springs. SMART Coil is a registered trademark of Dynamet Holdings, Inc. licensed to Dynamet Incorporated. Beta C is a registered trademark of RMI Corporation. Table 1 Minimum Specified Tensile Properties of Age- Hardened Material Diameter Tensile strength...