Alloy Digest (2001) 50 (8): Ti-117.
Published: 01 August 2001
... fracture toughness hardness high-temperature alloys physical properties RMI 5Al-2Zr-2Sn-4Mo-4Cr (Ti-17) tensile properties thermal properties UNS R58650 Ti-17 alloy is an -rich near- alloy that is sometimes classified as an alloy. Unlike other or near- alloys, Ti-17 offers good creep...