Alloy Digest (1981) 30 (1): Ti-81.
Published: 01 January 1981
... RMI 55 is a grade of commercially pure unalloyed titanium. It has good ductility and formability with a guaranteed minimum yield strength of 55,000 psi. It has good impact properties at room temperatures and excellent resistance to corrosion by marine atmospheres and seawater. Among its uses...
Journal Articles
Alloy Digest (1982) 31 (2): Ti-84.
Published: 01 February 1982
... RMI 8A1-1Mo-1V is an alpha-beta titanium alloy with a tensile strength of 135,000 psi in the mill-annealed condition. It has an excellent combination of tensile strength and creep resistance that makes it suitable for service to 1000 F. It is recommended for aircraft and jet-engine parts requiring...
Journal Articles
Alloy Digest (1981) 30 (8): Ti-83.
Published: 01 August 1981
... RMI 6Al-2Sn-4Zr-2Mo is an alpha-beta titanium alloy that provides a tensile strength of 130,000 psi in the mill-annealed condition. It is characterized by an excellent combination of tensile strength, creep strength, toughness and high-temperature stability that makes it suitable for service...
Journal Articles
Alloy Digest (2021) 70 (6): Ti-179.
Published: 01 June 2021
... (5.6)(b) 16 (9.25)(b) 0.42 0.52 (253 313)(b) RT = room temperature. (a) Source: Titanium Alloy Guide, RMI Titanium Company, Source: Titanium Alloy Guide, RMI Titanium Company, 2000, p 19 2000, p 19. (b) Source: Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Volume 2, ASM...
Journal Articles
Alloy Digest (2002) 51 (9): Ti-130.
Published: 01 September 2002
.... A specialized application for this alloy is aircraft springs. SMART Coil is a registered trademark of Dynamet Holdings, Inc. licensed to Dynamet Incorporated. Beta C is a registered trademark of RMI Corporation. Table 1 Minimum Specified Tensile Properties of Age- Hardened Material Diameter Tensile strength...
Journal Articles
Alloy Digest (2020) 69 (6): Ti-167.
Published: 01 June 2020
... (a) Source: RMI Titanium Company At 20 25 °C (68 78 °F) 20 100 °C (68 212 °F) 20 300 °C (68 572 °F) 20 500 °C (68 932 °F) 20 25 °C (68 78 °F) 20 25 °C (68 78 °F) Value 1660 (3020)(a) 921 (1690) 4510 (0.163) 8.6 (4.8) 9.5 (5.3) 9.7 (5.4) 21.8 (12.6) 519 (0.124)(a) 0.54 (321) Nonmagnetic Mechanical...