Journal Articles
Alloy Digest (1953) 2 (6): Cu-9.
Published: 01 June 1953
... REVERE No. 240 is a highly leaded brass combining free-machining characteristics with good mechanical and corrosion resistant properties suited to high-speed production in automatic screw machines. This datasheet provides information on composition, physical properties, hardness, elasticity...