Skip Nav Destination
Close Modal
Search Results for
REPUBLIC-70
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 33 Search Results for
REPUBLIC-70
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (9): SA-104.
Published: 01 September 1960
... REPUBLIC-70 is a precipitation hardenable low alloy steel which will meet 70,000 psi minimum yield point in the as-rolled condition followed by a precipitation hardening heat treatment. This datasheet provides information on composition, hardness, and tensile properties. It also includes...
Abstract
View article
PDF
REPUBLIC-70 is a precipitation hardenable low alloy steel which will meet 70,000 psi minimum yield point in the as-rolled condition followed by a precipitation hardening heat treatment. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-104. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (5): SA-372.
Published: 01 May 1980
... 200-600°F) 7.1 x 10-6 Thermal conductivity, Btu/ft 1 /in./hr/OF (At 70°F) 30 Modulus of elasticity, psi (Tension) 28-30 x 106 PROPERTIES Table 1 - MECHANICAL PROPERTIES (All data are for as-hot-rolled bars) Heat Treatment: Republic X-80-W Property Tensile strength, psi Yield strength (0.2% offset...
Abstract
View article
PDF
REPUBLIC X-80-W is a high-strength, low-alloy steel developed to achieve a minimum yield strength of 80,000 psi in the as-hot-rolled condition. It also exhibits good fatigue performance, good bendability, and good weldability. It is available as bars and can be used in various automotive and machinery applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-372. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (8): SA-307.
Published: 01 August 1974
...: Carbon Manganese Phosphorus Sulfur Silicon Nickel Chromium Molybdenum Copper Aluminum Typical 0.16 1.40 0.015 0.010 0.25 1.40 1.40 0.45 0.70 0.04 Physical Constants: (Approx.) Density, lb/cu in. Specific gravity Specific heat, Btu/lb/oF (70-2120F) Thermal coef. expansion/of (70-212oF) (704OOoF) (70~5720F...
Abstract
View article
PDF
REPUBLIC 100-AR was developed to provide a minimum yield strength of 100,000 psi in the as-rolled condition. It also has exceptional wear resistance, good toughness and design flexibility. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-307. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (5): SA-98.
Published: 01 May 1960
... ROLLED PROPERTIES Plate Thickness inch l/4 5J16 Plate Thickness inch l/4 5/16 318 l/2 Tensile Yield StMlgth Point psi psi 83400 53900 81400 57800 78900 58100 78000 59100 Elongation Brinell 70 in 2" Hardness 26.0 172 29.0 165 24.0 156 26.0 153 Table 2 - TYPICAL PRECIPITATION HARDENED PROPERTIES Tensile...
Abstract
View article
PDF
REPUBLIC-65 is a precipitation hardenable low alloy steel which will meet 65000 psi minimum yield point in the as-rolled condition followed by a precipitation hardening heat treatment. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-98. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (11): SA-170.
Published: 01 November 1964
... Modulus of elasticity, psi x 106 29-30 PROPERTIES Table 1 - TYPICAL HEAT TREATED PROPERTIES (Austenitized 1650oF, water quenched, tempered) Tensile Yield Reduction Strength Strength Elongation of Area psi psi (0.2%) Yc in 2 I ol . O 165000 15 5000 18 65 140000 125000 20 70 Table 2 - TYPICAL IMPACT DATA...
Abstract
View article
PDF
Republic HP150 is an alloy steel designed to give 150,000 psi yield strength with exceptional toughness. The alloy is intended for fabrication in the heat treated condition principally for heavy plate sections. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-170. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1963) 12 (7): SA-149.
Published: 01 July 1963
... 39000 - 30 7.82 0.282 6.3 28-30 12 Drilling is performed with high speed steel drills of standard design at cutting speed of 70-90 sfpm for inch drills. Smaller drills require slightly slower speeds. Milling with high speed steel cutters can be dooe at 90-130 .sfPm for face milling and 60-90 sfpm...
Abstract
View article
PDF
Republic-M is a low carbon, manganese type structural steel having high notch-impact resistance and high ductility at subzero temperatures. It is recommended for structural applications where weight reduction is important. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-149. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (10): Ti-7.
Published: 01 October 1955
... 1000 1000 1100 1100 1200 1200 1300 1300 Tensile strength, psi Yield strength (0.2%) psi Elongation, 70 in 2 khlctLlof Minimum Typical 150,000 161,000 140,000 10 15::oo $7 Table 2 - CHARF Y IMPACT vs TEMPERATURE (Average Values 3/q Barstock) Temperature OF. -rt l~pm . . -200 9 -100 0 :: 100 14 200 16...
Abstract
View article
PDF
REPUBLIC RS-140X is a titanium alloy containing iron, chromium and aluminum as its principal alloying additions. It is primarily a bar and forging alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ti-7. Producer or source: Republic Steel Corporation, Titanium Division.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (7): SA-179.
Published: 01 July 1965
... Elongation of Area Brine11 oF psi psi (0.2%) 70 in 2 tr, Hardness 400 290000 250000 -, 30 543 600 250000 235000 ; 40 469 (Austenitized 1450oF, quenched in salt at 475oF, held at temperature for 7 hours, air cooled) Transformation Temperature, oF 475 270000 225000 10 40 534 Table 2 - IMPACT DATA...
Abstract
View article
PDF
Republic HP 9-4-45 is a heat treated alloy steel capable of developing a yield strength of 250,000 psi with superior toughness characteristics. It is designed for sheet and thin-walled forged sections. It is also designed for heavy forging where an isothermal heat treatment is employed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-179. Producer or source: Republic Steel Corporation, Titanium Division.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (11): Ti-42.
Published: 01 November 1964
... 33000 20000 1200 14000 5000 4.46 0.161 0.153 16-18 0.0001573 5.2 4.31 6.30 10.48 DOI: 10.31399/asm.ad.ti0042 Copyright © ASM International® 1996 Table 4 - ELEVATED TEMPERATURE PROPERTIES - Annealed Shea Temperature oF 70 200 400 600 800 1000 Tensile Yield Strengcb Strength psi psi (0.2%) 136ooo 124000...
Abstract
View article
PDF
Republic RS-110C is a moderate strength highly weldable titanium alloy recommended for jet engine welded rings, aircraft skins, and structural parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-42. Producer or source: Republic Steel Corporation, Titanium Division.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (8): SA-242.
Published: 01 August 1969
.... high-strength bolts, etc. Composition: Carbon Nickel Cobalt Molybdenum Titanium Iron 0.03 max. 18-19 8.0-9.5 4.6b5.20 0.50-0.85 Remainder Physical Constants: Specific gravity Density. Ib/cu.in. Thermal coef. expansion/OF (70-900oFj Electrical resistivny. microhms-cm (agedj Modulus of elasticity, psi...
Abstract
View article
PDF
Republic RSM-300 alloy is an 18% nickel-cobalt-molybdenum age-hardening steel designed to develop up to 300,000 psi yield strength with good toughness. It is recommended for landing gears extrusion dies, rocket motor cases, high-strength bolts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as heat treating, machining, joining, and surface treatment. Filing Code: SA-242. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (3): SA-250.
Published: 01 March 1970
... Constants: (maraged) Specific gravity Density, Ib./cu. in. Thermal ccef. expansion/of (70-900oF) Electrical resistivity, microhms-cm Modulus of elasticity, psi Modulus of rigidity, psi 8.00 0.29 5.6x10-6 38-39 26.5-27.5x106 10.2~106 Poisson s ratio 0.30 PROPERTIES Table 1 - TYPICAL ROOM TEMPERATURE...
Abstract
View article
PDF
REPUBLIC RSM 250 is an 18% nickel-cobalt-molybdenum age-hardening steel designed to develop 250,000 psi yield strength with good toughness. It is recommended where a combination of strength, toughness and notch resistance is required such as aircraft landing gears and jet engine components. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-250. Producer or source: Republic Steel Corporation, Titanium Division.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (1): SA-353.
Published: 01 January 1979
... values). *LOCORE is a registered trademark of Republic Steel Corporation. Composition: l Carbon Silicon Iron Approximate Range ** 1.20-l .70 Remainder Physical Constants: (Approximate) Density, g/cu cm (At 2OoC) lb/cu in. (At 680F) Thermal conductivity, cal/cm2/cm/s/oC (At 200C) Electrical resistivity...
Abstract
View article
PDF
LOCORE M45 is a cold-rolled, non-oriented electrical steel used primarily for alternating current (AC) and direct current (DC) motors, generators and transformers. It is produced either semiprocessed (the consumer anneals to produce the desired magnetic properties) or fully processed (the steel producer develops the magnetic properties to meet the maximum core loss values). This datasheet provides information on composition, physical properties, microstructure, and elasticity. It also includes information on heat treating and joining. Filing Code: SA-353. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (1): SA-312.
Published: 01 January 1975
.... expansion/OF (70-2OOoF) (200-6OOoF) Electrical resistivity. microhm-cm (At 70oF) hlodulus of elasticity. psi (Tension) 0.283 7.83 0.116 0.124 30.0 29.5 6.8 s 10-6 7.1 s 10-6 15.5 29-30 x 106 optional on a heat lot basis for improved atmospheric corrosion resistance. PROPERTIES Table 1 - MECHANICAL...
Abstract
View article
PDF
MAXI-FORM 80 is a high-strength low-alloy steel that provides superior ductility, good fatigue resistance, good weldability and outstanding impact toughness even at temperatures down to -40 F and below. It has a yield strength of 80,000 psi along with the high formability that complex parts require. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-312. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1962) 11 (10): SS-137.
Published: 01 October 1962
... hardness 145-210 Rockwell hardness BSO-95 Charpy impact, ft. lbs. 35-70 Table 2 - STRESS-RUPTURE PROPERTIES Test TemTmre Stress, psi for Rupture in 100 hrs. 1000 hrs. 10,000 hrs. 1000 32000 16000 1200 26000 14000 9000 1400 11500 5100 4000 1600 ROOO 2400 1500 1800 2000 800 Table 3 - TYPICAL ELEVATED...
Abstract
View article
PDF
ENDURO NC-3 is a chromium-nickel heat and corrosion resistant steel of the Type 310 grade. It is austenitic and nonmagnetic. It meets the need for an alloy that will resist greater stress and oxidation at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-137. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (8): SS-185.
Published: 01 August 1966
..., cutlery, pump components, etc. Composition: Carbon Manganese Silicon Sulphur Phosphorus Chromium Iron 0.15 max. 1.00 max. 1.00 max. 0.03 max. 0.04 max. 11.5-13.5 Remainder Physical Constants: (at 70°F) Specific gravity Density, lb/cu.in. Specific hear, Bcu/lb/OF (0-200°F) Thermal conductivity, Bcu...
Abstract
View article
PDF
ENDURO S-1 is a chromium type stainless steel providing high strength, toughness and resistance to impact when heat treated. It shows resistance to wet and dry corrosion. It is recommended for steam turbine parts, valves, cutlery, pump components, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-185. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (2): SS-25.
Published: 01 February 1955
...-1600 F., cool slowly in air. HARDEN: Not hardenable by thermal treatment. Machinability: Its machinability raring is about 50-70s of that of AISI B1112 steel The machinability is best when it is slightly hardened by cold work such as cold rolling. In spite of the higher chromium content the machin...
Abstract
View article
PDF
ENDURO HC is a high chromium heat and corrosion resisting steel of the AISI Type 446 grade. It is magnetic and cannot be hardened materially by heat treatment. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-25. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (6): SS-118.
Published: 01 June 1961
...-210000 Yield point, psi 90000-170000 Elongation, % in 2 20-15 Reduction of area, % 65-50 lzod impact, ft. lbs. 70-15 Brine11 Hardness 250-415 Rockwell hardness C22-43 Table 4 - TYPICAL HEAT TREATED PROPERTIES - 1 Bar (Oil quenched from 1750oF. tempered 2 hours) Tensile Yield Reduction Streogth Strength...
Abstract
View article
PDF
Enduro S-1 Nickel is a martensitic type stainless steel combining good corrosion and heat resistance with high strength and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-118. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (8): SS-46.
Published: 01 August 1956
.... Melting point, OF. Ekcctical tesistiviy, mictohm-cm at 70°F. Modulus of eIasticity in tension x 106 psi 7.73 0.28 0.11 ::z 2.: 2 700-2790 57.0 29.0 PROPERTIES Table 1 - TYPICAL MECHANICAL PROPERTIES - BARS 1 DIAMETER AnneaIed Heat Treated Tempered & Cold Drawn Tensile sttength, psi 75000 110000 100000...
Abstract
View article
PDF
ENDURO FC is a free-machining chromium type stainless steel equivalent to AISI Type 416. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-46. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (10): SS-35.
Published: 01 October 1955
...& gravity Density, Ib./cu.in. Specific heat, BTU/lb/F. (O-200°F.) Thermal conductivity! Bl$I/ft/hr/ F./io. (200°F.) Thermal coef. ;rp~i~/ F. 0:600 F: O-1500°F. Melting point, F. ElectricaI resistiviy, microhms/in3 (70°F.) Modulus of elasticity, psi Magnetic permeability (anneakd) PROPERTIES Table 1...
Abstract
View article
PDF
ENDURO AA-FM is a free-machining chromium type stainless steel equivalent to AISI Type 430-F. It is ferritic and non-hardenable. It is corrosion and heat resistant. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-35. Producer or source: Republic Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1953) 2 (6): SS-9.
Published: 01 June 1953
... - Brine11 hardness 140-160 185 Table 2 TYPICAL PROPERTIES - ANNEALED CONDITION Sheet Soft Wire and Strip 0.250" Plate Tensile strength, psi 75000 70000 75000 Yield strength, (.2% set) psi 45000 40000 40000 Elongation, % io 2 25 35 30 Reduction of area, % - 70 - Brine11 hardness. 3000 Kg. - B; 160 Rockwell...
Abstract
View article
PDF
ENDURO AA is a ductile, non-hardening alloy containing 14 to 18 percent chromium with carbon under 0.12 per cent. It has mechanical properties equal to high grade medium carbon steel, with high resistance to general corrosion and oxidation at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-9. Producer or source: Republic Steel Corporation.