1-18 of 18 Search Results for

REPUBLIC-65

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (5): SA-98.
Published: 01 May 1960
... REPUBLIC-65 is a precipitation hardenable low alloy steel which will meet 65000 psi minimum yield point in the as-rolled condition followed by a precipitation hardening heat treatment. This datasheet provides information on composition, hardness, and tensile properties. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (12): SS-65.
Published: 01 December 1957
... properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-65. Producer or source: Republic Steel Corporation...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (11): SA-170.
Published: 01 November 1964
... Modulus of elasticity, psi x 106 29-30 PROPERTIES Table 1 - TYPICAL HEAT TREATED PROPERTIES (Austenitized 1650oF, water quenched, tempered) Tensile Yield Reduction Strength Strength Elongation of Area psi psi (0.2%) Yc in 2 I ol . O 165000 15 5000 18 65 140000 125000 20 70 Table 2 - TYPICAL IMPACT DATA...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (5): SA-372.
Published: 01 May 1980
... equals thickness or diameter) in the longitu- dinal direction can be assured on both flat and round bars. Minimum Typical Range 95000 97000- 120000 80000 82000-95000 - 0.75-0.80 18 20-33 - 55-65 Weldability: Both laboratory and customer field experience have confirmed that Republic X-80-W can be fillet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (12): SA-270.
Published: 01 December 1971
..., psi 19500@215000 Yield strength (0.2% offset), psi 18000~195000 Elongation (2 in. or 4D), 5 14-19 Reduction of area, s 55-65 Charpy impact (V-notch), ft-lb 45-60 Klc (Notch bend), psi 6 150000 Yield strength (0.270 offset), psi (compression) 202000 Fatigue strength* (107 cycles), psi (No notch) 112000...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (11): Ti-42.
Published: 01 November 1964
... STRENGTH - Bar Temperacure, oF Charpy Impact, ft. lbs. *Extrapolated 17 18 20 26 40 49 56 65 75. 90. Table 3 - STRESS-RUPTURE PROPERTIES - Annealed Sheet Temperacure Stress, psi co produce Rupture in oF 10 hrs. 1000 hrs. 80 104000 100000 200 96000 94000 400 79000 76000 600 67000 65000 800 62000 58000 1000...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (7): SA-179.
Published: 01 July 1965
... 290000 250000 140000 260000 50 0.180 290000 250000 110000 170000 600 0.080 250000 235000 170000 250000 2; 0.180 250000 235000 165000 245000 65 Isothermal Treatment,oF (Bainite) 475 0.080 27 0000 225000 200000 270000 100 0.180 270000 225000 190000 245000 100 *Fatigue cracked center-notched specimens...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (5): SA-209.
Published: 01 May 1967
... Reduction of area, S 65-75 Rockwell hardness C28-30 Table 2 - TYPIC.\L MARAGED PROPERTIES (.Jnnealed, then maraged at 900┬░F for 3 hours) Tensile strength, psi 210000 Yield strength, psi (0.2%) 200000 Elongation, % in 2 14 Reduction of area, % 55 Notch T.S. to T.S. ratio* 1.60 Endurance limir, psi (10...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (8): SA-242.
Published: 01 August 1969
... in. IS-20 Reduction of area, % 65-75 Rockwell hardness C28-30 Table 2 - TYPICAL MARAGED PROPERTIES (Annealed, then maraged at 9OOoF for 3 hours) Tensile strength, psi 265000-305000 Yield strength. psi (0.25,) 26000@300000 Elongation, % in 2 in. 3-10 Reduction of area, c*c 20-50 Notch T.S. to T.S. ratio...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (6): SS-118.
Published: 01 June 1961
...-210000 Yield point, psi 90000-170000 Elongation, % in 2 20-15 Reduction of area, % 65-50 lzod impact, ft. lbs. 70-15 Brine11 Hardness 250-415 Rockwell hardness C22-43 Table 4 - TYPICAL HEAT TREATED PROPERTIES - 1 Bar (Oil quenched from 1750oF. tempered 2 hours) Tensile Yield Reduction Streogth Strength...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (2): SS-25.
Published: 01 February 1955
... - TUBING AND WIRE PROPERTIES Tubing Wire Anneals Cold Drawn 65% 83000 135000 55000 115000 25 50 175 Table 3 - BAR AND ROD PROPERTIES Forged, Rolled and Annealed 75000-95000 45000-60000 25-35 45-65 160-200 0.050 0.058 0.0000058 0.0000063 29,000,000 Plate Annealed 85000 55000 25 B83 180 2 Wire Annealed 90000...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (8): SS-185.
Published: 01 August 1966
... strength, psi Yield point, psi Elongation, % in 2 Reduction of area, % Brine11 hardness Rockwell hardness Izod impact, fc. Ibs. Olsen ductility, in. 6500085000 35000-50000 35-20 65-80 135-165 B75-85 100-60 0.350-0.275 90000-120000 70000-90000 13-17 55-65 187-248 B90- 100 Table 2 - CHARPY IMPACT PROPERTIES...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1962) 11 (10): SS-137.
Published: 01 October 1962
...-2650 Modulus of elasticity, psi I 106 30.5 Electrical resisciviry, microhms/in3 30.5 Magnetic permeability 1.001 PROPERTIES Table 1 - TYPICAL MECHANICAL PROPERTIES - Annealed Tensile strength, psi 90000-l 10000 Yield point, psi 40000-60000 Elongation, % in 2 45-55 Reduction of area, % 50-65 Brine11...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (8): SS-46.
Published: 01 August 1956
... 30-20 25-15 65-60 60-40 138-160 B80-90 1 SO-300 ClO-30 95-70 100-10 Table 4 - CREEP STRENGTH (for a life of 10,000 hts. with 1% elongation) Tempenuute. OF. Creep Strength, psi 1000 12500 1100 5000 1200 2100 1300 1400 Tempering Tensile Sttengch Temperature, OF. psi 300 5 :i%fl 700 900 :zKz 1000 145000...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (4): SS-207.
Published: 01 April 1968
... TEMPERATURE PROPERTIES fAnnealed material) Test Tensile Temperature Strength OF psi 0 96000 -100 118000 -200 145000 -300 175000 -400 215000 Yield Screnath Elongation psi (O.Z%) % ii 2 45000 67 55000 65 68000 62 78000 59 89000 56 Annealed 80000-90000 35000-55000 70-50 7560 135-185 B70-90 120-70 Cold Rolled...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (2): SA-343.
Published: 01 February 1978
... and low-alloy steels. Specification Equivalents: AhIS 6524. AhlS 65 26. AMD 65CE. ASTM A 579, Grade 82. General Characteristics: Lescalloy HP 9430 Vat-Arc is a nickel-cobalt hardenable low-alloy steeL It is normally austenitized, quenched to mar- tensite and tempered to provide the desired properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (11): Ni-692.
Published: 01 November 2011
...) 620 (1148) 220 (31.9) 155 (22.5) 640 (1184) 185 (26.6) 133 (19.3) 660 (1220) 160 (23.2) 119 (17.2) 680 (1256) 141 (20.4) 107 (15.5) 700 (1292) 123 (17.8) 95 (13.8) 720 (1328) 109 (15.8) 83 (12.0) 740 (1364) 96 (13.9) 71 (10.3) 800 (1472) 65 (9.4) 43 (6.2) ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (6): SS-156.
Published: 01 June 1964
... sfpm in automatic screw machines has been used. In the harden- ed condition the alloy can be machined ac races approxi- macely 60% of chose for annealed material, however, compared co AISI B 1112 Bessemer screw stock, solution created No. 630 has a machinability racing of about 65 per cent. Single...