Alloy Digest (1995) 44 (12): SS-628.
Published: 01 December 1995
... REMANIT 4510 is a ductile non-hardenable type of stainless steel recommended for parts requiring a combination of good formability, weldability and corrosion resistance. This composition is a modification of Type 430 with an addition of titanium. This addition helps in corrosion resistance making...