... REMANIT 4462 is a ferritic/austenitic duplex stainless steel with a low carbon content, an addition of nitrogen and a balanced ratio of the alloying elements. This offers a stable structure with good weldability. REMANIT 4462 is well suited for many applications in the chemical industry, in off...
Journal Articles
Alloy Digest (2004) 53 (5): SS-903.
Published: 01 May 2004
... Hyresist 22 Industeel UR 45N Valourec VS 22 Bohler A903 Edelstahl Witten-Krefeld Remanit 4462 Mannesmann AF22 (1.4462) ThyssenKrupp VDM Cronifer 2205LCN Krupp Edelstahlprofile Falc 223 Schmidt & Clemens Maresist F51 (cast) Sumitomo SM22Cr Nippon Kokan NkCr22 plus the following 25%Cr Mo-free alloys UNS...