1-12 of 12 Search Results for

REFRACTORY SHEET TYPE 100

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1991) 40 (10): Cp-19.
Published: 01 October 1991
... Refractory Sheet Type 100 is an engineered ceramic, fiber reinforced structural alumina composite with useful properties in thermal, structural and electrical insulation applications; as well as the transport of molten nonferrous metals to 1260 C (2300 F). This datasheet provides information...
Journal Articles
Alloy Digest (1974) 23 (7): Ta-4.
Published: 01 July 1974
... of the cutting tool. To reduce cratering and abrasive wear, high positive rake angles should be employed whenever possible and a water soluble coolant with good lubricity and wetting characteristics should be used. For rough turning, use AISI Type M-36 or T-5 cutting tools with cutting speeds of 50 to 100 sipm...
Journal Articles
Alloy Digest (1964) 13 (12): W-8.
Published: 01 December 1964
... and liberal application of the cooling media should be employed. Silicon carbide wheels are most satisfactory for all types of grinding. Ingots can be sawed with a power hacksaw or a hand saw. However, this is a difficult operation and blades dull quickly. .4ir often improves sawa- bility more than liquid...
Journal Articles
Alloy Digest (1965) 14 (8): W-9.
Published: 01 August 1965
... for all types of grinding. General Characteristics: OREMET 85W-15Mo centrifugal castings are 100% dense, fine grain homogeneous alloy of tungsten- molybdenum. It has excellent mechanical proper- ties at elevated temperatures. The oxidation rate at 175OoF in air is approximately 0.30 gm/cm /hr. weight loss...
Journal Articles
Alloy Digest (1984) 33 (3): Ta-7.
Published: 01 March 1984
...). PROPERTIES Table 1 -GRAIN SIZE AND TENSILE PROPERTIES KBI-40 Tantalum Average grain size, ASTM scale 8-9 6-7 (0.030-in. thick sheet) Tensile strength, psi. min 40000 30000 Yield strength (0.2qlc offset), psi. min 28000 20000 Elongation (2 in TO. min 25 25 Heat Treatment: Full anneal: In general, heat to Il5O...
Journal Articles
Alloy Digest (1982) 31 (4): Ta-5.
Published: 01 April 1982
...-WORKED FANSTEEL 63 METAL Material for Annealing: Reduction by cold rolling 0.250-inch plate, 070 68 76 84 88 92 96 97 Sheet thickness, inch 0.080 0.060 0.040 0.030 0.020 0.010 0.007 Temp., C. for 95 + % recrystallization I200 1200 1200 I200 II50 1150 1150 Resulting ASTM Grain Size No. 6 6% 6% 7 7 7 7...
Journal Articles
Alloy Digest (1994) 43 (3): Hf-1.
Published: 01 March 1994
... Magnesium Manganese Nickel Nimogen Oxygen Silicon Titanium Uranium Zirconium Copper Molybdenum Tungsten Columbium Hydrogen Tantalum Vanadium Sponge crystal Rod & Sheet, Plate Bar Wire & strip - - 200 70 100 100 100 30 150 150 200 100 20 100 100 750 250 250 250 600 50 50 50 50 50 50 10 100 100 1500 100 400...
Journal Articles
Alloy Digest (1970) 19 (10): Mo-10.
Published: 01 October 1970
... in producing a good machine fmish. Choice between high-speed steel and sintered carbide tools depends largely on production quantities. High-speed steel tools are generally used for small quantities or for roughing cuts. The preferred carbide grades are the straight tungsten-carbide-cobalt types recommended...
Journal Articles
Alloy Digest (1963) 12 (9): Cb-5.
Published: 01 September 1963
... requiring extended use at elevated remperarures in an oxidizing environment. The weight gain in staric air al 20000F is 39.0 mg/cm2, hr. (0.020 chick B-66 coated with Sylcor (an Al-Sn dip-type coating) aithstood one hour exposure ar 25000F in static air wirhour failure.) B-66 has demonsrraced...
Journal Articles
Alloy Digest (2020) 69 (10): SS-1328.
Published: 01 October 2020
... temperature strength than the common austenitic stainless steels such as Type 304. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing...
Journal Articles
Alloy Digest (2020) 69 (5): SS-1318.
Published: 01 May 2020
... of room temperature strength than the common austenitic alloys such as Type 304. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SS-1318. Producer...
Journal Articles
Alloy Digest (2007) 56 (10): SS-998.
Published: 01 October 2007
... and vertical centrifugal castings; static castings Applications: Applications include ammonia, methanol, and hydrogen reformers; ethylene pyrolysis coils and fittings; steam superheater tubes and fittings; tube supports and hangers; tube sheets; heat treatment fixtures and trays; refractory supports; furnace...