1-20 of 21 Search Results for

RED CUT SUPERIOR J

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1983) 32 (1): TS-410.
Published: 01 January 1983
... RED CUT SUPERIOR J is a tungsten-type of hot-work tool and die steel; in fact, it is the 18 tungsten-4 chromium-1 vanadium high-speed composition with carbon lowered to provide more toughness. It is characterized by high red hardness and good resistance to abrasion. It is recommended...
Journal Articles
Alloy Digest (1959) 8 (11): TS-86.
Published: 01 November 1959
... CARPENTER No. 883 is a 5% chromium hot work steel designed particularly for applications requiring extreme toughness combined with good red-hardness. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and creep. It also includes...
Journal Articles
Alloy Digest (2006) 55 (11): TS-304.
Published: 01 November 2006
... Material annealed to a hardness of 285 311 HB. The machinability is approximately 15% that of B1112 steel. superior to that of M42. With its high hardness, fine grain size, and uniform carbide distribution, CPM Rex 76 is used for special- purpose cutting tools requiring high red hardness, high abrasion...
Journal Articles
Alloy Digest (2007) 56 (3): TS-249.
Published: 01 March 2007
... is ideal for cutting difficult-to-machine material where high frictional heating is encountered. The CPM process results in a homogeneous microstructure with a finer, more uniform carbide distribution imparting superior dimen- sional stability, grindability, and toughness when compared to steels produced...
Journal Articles
Alloy Digest (1956) 5 (12): Cu-45.
Published: 01 December 1956
... is superior to yellow brass. Pickling: The oxide normally formed during anneal is particular- ly tenacious and the usual brass mill pickle solution containing 10.20% sulphuric acid leaves the alIoy with a thin oxide coating of dark red color. This red oxide surface is highly satisfactory for many uses...
Journal Articles
Alloy Digest (1962) 11 (1): Co-6.
Published: 01 January 1962
..., Inc. Upper MO-. New J=~Y REXALLOY@ 33 (Hard, Wear Resistant Alloy) REXALLOY jj is a cast non-ferrous cobalt-base alloy of chromium, tungsren and carbon which is recommended for cut- ring cools and wear-resistant parts. Composition: Carbon 2.25 8.78 rungsten 17.00 0.317 Chromium 33.00 39.8 Cobalt 44.dO...
Journal Articles
Alloy Digest (1967) 16 (1): TS-188.
Published: 01 January 1967
... VERSASTEEL Tool stool JANUARY 1967 -DATA ON WORLD WIDE METALS AND ALLOYS p*uirbJ by Engineahlg Alloys Dwtl IfK. VERSASTEEL Upper Moaadrir. New J~=Y (High-Carbon Alloy Tool Steel) VERSASTEEL is a tool steel designed co provide an unusual combination of fine grain S~~CN~C, high secoodary hardness...
Journal Articles
Alloy Digest (2021) 70 (9): SS-1339.
Published: 01 September 2021
... CarTech 347 is a niobium+tantalum stabilized austenitic stainless steel. Like Type 321 austenitic stainless steel, it has superior intergranular corrosion resistance as compared to typical 18-8 austenitic stainless steels. Since niobium and tantalum have stronger affinity for carbon than chromium...
Journal Articles
Alloy Digest (1967) 16 (5): TS-193.
Published: 01 May 1967
... Filing Code: TS-193 Tool Steel MAY 1967 BIQ#ST -DATA ON WORLD WIDE METALS AND ALLOYS AlSl Type H13 (Hot Work Tool Steel) Engiaeeriag Alloys Digest, Inc. Upper MotttcU New J-w AIs1 Type H13 is an air-hardening hoc work tool and die steel having a high resistance to heat checking has good wear resistance...
Journal Articles
Alloy Digest (2002) 51 (5): Ti-127.
Published: 01 May 2002
... Carpenter CP Titanium Grade 2 is intermediate in strength when compared to the unalloyed grades 1-4. The alloy is widely used because it combines excellent formability and moderate strength with superior corrosion resistance. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1962) 11 (6): SA-130.
Published: 01 June 1962
... Latrobe AGT Vac-Arc is a chromium-nickel-molybdenum alloy case hardening steel of superior cleanliness and uniform quality, recommended where high tensile and fatigue strengths are required with high shock resistance. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1993) 42 (8): Co-93.
Published: 01 August 1993
... solder, 0.003 to 0.005 in. (0.076 to 0.122 mm) thick, cut slightly oversize, are positioned be- tween the parts. The materials are then treated to cherry red in an induction coil. a furnace or with a slightly reducing oxy- acetylene flame. As soon as the silver alloy melts, the source of heat is removed...
Journal Articles
Alloy Digest (1954) 3 (11): TS-27.
Published: 01 November 1954
... obtainable with these tools jusrify a broader appiicarion and resuit in more econ- omicai production. The superior cutting properties make it possible to machine exaemely hard mauziak suchaschilledro~,ha~aatedparrs,asw~ascast iron and heavily scaled flashings where the cool is subjected to extreme wear...
Journal Articles
Alloy Digest (2016) 65 (1): SA-740.
Published: 01 January 2016
... carbide tool Sandvik SNMG 120408-PM- 4015 Feed 0.4 mm/rev (0.02 in./rev) Cutting depth 2 mm (0.08 in.) Wear criterion 0.4 mm (0.02 in.) Cutting fluid: Peralube 0125 5% See Fig. 1. Specific machining recommendations of turning and threading of this alloy are tabulated in Table 2. Copyright © 2016...
Journal Articles
Alloy Digest (1960) 9 (2): TS-89.
Published: 01 February 1960
... with these tools justify a broader application and result in more economical production. The superior cutting possible to machine extremely har 1 roperties make it materials such as chilled rolls, heat treated parts, as well as cast iron and heavily scaled flashings where the tool is subjected to extreme wear...
Journal Articles
Alloy Digest (1970) 19 (6): SA-253.
Published: 01 June 1970
... or rolled specimens only: Normalize 17OOoF) (Austenitize 17OOoF) J Distance Rockwell C Sixteenths Hardess Limits of an Inch Max Mill : :i 45 : 43 36 ;i 24 2 31 21 ii 24 :: - 9 :: E - 12 I: - 13 :: 16 :A 7.82 0.283 0.080 0.147 25.5 6.5 x 10-6 7.0x 10-6 7.7 x 10-6 20 29-30 x 106 DOI: 10.31399/asm.ad.sa0253...
Journal Articles
Alloy Digest (1982) 31 (3): Ni-274.
Published: 01 March 1982
... alloy No. N-6 should be evaluated for applications such as fluid valves, corn-cutting knives, glass-shearing blades and automatic applications where STELLITE alloy No. 6 has been used successfully. This datasheet provides information on composition, physical properties, and hardness as well as fracture...
Journal Articles
Alloy Digest (1965) 14 (8): TS-168.
Published: 01 August 1965
... tensile properties workability AN Type A2 Filing Code: TS-168 Tool Steel AUGUST 1965 -DATA ON WORLD WIDE METALS AND AL- - _ - AISI Type A2 (Air Hardening Tool Steel) Prblisbd by Engioeering Alloys Digest, Inc. Upper Mantdsir, Neo* J==Y AISI Type-A2 is a high-carbon, chromium, molybdenum tool and die...
Journal Articles
Alloy Digest (2006) 55 (12): TS-639.
Published: 01 December 2006
... Hardening temperature Tempering temperature Impact toughness, Charpy C-notch Bend fracture strength °C °F °C °F Hardness, HRC J ft . lbf MPa ksi 1205 2200 550 1025 65.5 27 20 5088 738 1165 2125 565 1050 63.5 38 28 5129 744 Depending on the hardness requirement, lowering the hardening temperature...
Journal Articles
Alloy Digest (1960) 9 (12): SS-112.
Published: 01 December 1960
... tensile properties workability ALLEGHENY METAL 355 Filing Code: SS-112 Stainless Steel DECEMBER 1960 I I -DATA ON WORLD WIDE METALS AND ALLOYS ALLEGHENY METAL 355 (Heat Treatable Stainless Steel) published by Engineering Alloys Digest. Inc. Upper Montclair, Near J~~ss Allegheny Metal 355 is a new type...