... RAFFMETAL EN AB-Al Si10Mg (EN AB-43000) is a heat-treatable, aluminum-silicon-magnesium casting alloy in ingot form for remelting. It is used extensively for producing sand and permanent mold castings for applications requiring a combination of excellent casting characteristics, high strength...