Alloy Digest (1972) 21 (12): Co-67.
Published: 01 December 1972
... RAECO-15 is a magnet alloy of samarium and cobalt which offers 15-million energy product, an extremely high intrinsic coercive force (Hci = 15,000 Oe), and a Curie Temperature of 750 C. It is especially attractive for use in severe demagnetizing environments at elevated temperatures...