1-2 of 2 Search Results for

Pyrotool V

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1971) 20 (12): Fe-49.
Published: 01 December 1971
... PYROTOOL V is an austenitic precipitation-hardenable iron-base alloy designed to display high-strength properties at temperatures up to 1300 F (704 C). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1972) 21 (4): SS-271.
Published: 01 April 1972
... PYROTOOL 15 is a low-carbon martensitic precipitation-hardenable (maraging) heat-resistant steel designed to possess high strength from room temperature to 1050 F. Uses include tooling applications. This datasheet provides information on composition, physical properties, hardness, elasticity...