1-4 of 4 Search Results for

Pyromet alloy CTX-1

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1997) 46 (5): Fe-56.
Published: 01 May 1997
... Pyromet CTX-1 is a high-strength, precipitation-hardenable superalloy exhibiting a low coefficient of thermal expansion and high strength up to about 1200 deg F. The alloy possesses high hot hardness and good thermal fatigue resistance. Its applications include components for gas turbine engines...
Journal Articles
Alloy Digest (1990) 39 (1): Fe-89.
Published: 01 January 1990
... thermal fatigue resistance. It offers significant improvement over Pyromet alloys CTX- 1 and CTX-3 with excellent tensile properties and stress-rupture strength in the recrystallized and aged condition. It is weldable, brazable and can be chromium plated. Forms Avallable: Bar, wire billet. Appllcatlons...
Journal Articles
Alloy Digest (1987) 36 (7): Fe-78.
Published: 01 July 1987
...) 2000 *ICI = 2, low-stress ground specimens. Properties are lowered if lathe- turned specimens are used. Heat Treatment: The optimum heat treatment for Pyromet CTX-3 varies with property requirements: Heat Treatment A: Warm-worked material is solution treated at 1800 F (98O C) for 1 hour and air cooled...
Journal Articles
Alloy Digest (1994) 43 (2): Fe-105.
Published: 01 February 1994
... hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, high tensile and rupture strengths, and good thermal fatigue resistance. This alloy offers a significant improvement in environmental resistance over Pyromet alloys CTX-1, CTX-3, and CTX-909 due to the...