Skip Nav Destination
Close Modal
Search Results for
Pyromet X-12
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 20 Search Results for
Pyromet X-12
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1964) 13 (2): SS-152.
Published: 01 February 1964
... Pyromet X-12 is a martensitic stainless steel offering high strength at both room temperature and high heat. It is recommended for use in jet engines, steam turbines and aircraft structural parts. This datasheet provides information on composition, physical properties, hardness, elasticity...
Abstract
View article
PDF
Pyromet X-12 is a martensitic stainless steel offering high strength at both room temperature and high heat. It is recommended for use in jet engines, steam turbines and aircraft structural parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-152. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1975) 24 (4): Ni-216.
Published: 01 April 1975
.... Machinability: The machinability of Pyromet 901 is best in the overaged condition; however, it can be machined when solution treated or fully aged. The machinability rating in the solution-treated condition at a BrineU hardness around 170 is about 25% of AK1 B 11 12. Single-point turning with high-speed-steel...
Abstract
View article
PDF
PYROMET 901 is a nickel-chromium super alloy designed for high strength and corrosion resistance in the temperature range of 1000-1400 F. Compounds of Ni3 (Al, Ti) type produce the precipitation hardening. It is used in a variety of high-temperature applications such as components in aircraft and gas turbines. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-216. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1987) 36 (7): Fe-78.
Published: 01 July 1987
... WIDE METALS AND ALLOYS JULY 1887 @coPyright 1987. Alloy DIgat. Inc. All ngbu -ed. ISSN:OO2dl4X hblishcd by: Alloy wt. Inc 27Caddd Sweet &!a horn are rypical. nor to be used for Jpeclficarron or/inai dmgn Oran& New Jersey 07050 (201)677-9161 PYROMET+ 0-X-3 (Low-Expansion Iron-Base Superalloy) PYROMET...
Abstract
View article
PDF
PYROMET CTX-3 is a high-strength precipitation-hardenable low-expansion superalloy. It exhibits a low coefficient of thermal expansion over a broad temperature range combined with high strength. The alloy possesses high hot hardness and good resistance to thermal fatigue. It is brazable, weldable and can be plated with chromium. CTX-3 uses comprise compressor and exhaust casings, seals and other components for gas turbine engines. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-78. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1977) 26 (6): SS-340.
Published: 01 June 1977
...) 12 29000 (200) 30 1350 732 35000 (241) 29 21000 (145) 35 1500 816 13000 (90) 55 7700 (53) 0.286 7.92 2500-2600 0.110 9.17 x 10-6 9.47 x 10-6 9.78 x 10-6 10.32 x 10-6 104.2 165.0 See Tables 1 & 2 1.010 1.007 Copyright © ASM International® 1996DOI: 10.31399/asm.ad.ss0340 Test Table 5 - CREEP STRENGTH...
Abstract
View article
PDF
PYROMET A-286 is an age-hardenable austenitic iron-nickel-chromium alloy designed for service up to 1300 F (704 C) on jobs requiring high strength and good corrosion resistance at the operating temperature. It offers high ductility in notched sections. Pyromet A-286 is used in jet engines and superchargers for various high-temperature components. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-340. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1989) 38 (8): Ni-185.
Published: 01 August 1989
... sections. Corrosion Resistance: Pyromet@ alloy 88 has good high-temperature corrosion x&s- tance under both oxidizing and reducing conditions. the alloy is highly resistant to engine exhaust gases. It is vulnerable to SldiidatiCRL General Characteristics: Pyromet@ alloy 88 is a high-strength nickel-base...
Abstract
View article
PDF
PYROMET alloy 88 is an age hardenable nickel-base alloy with high strength good corrosion and oxidation resistance. It possesses low creep rate in the temperature range 1200-1500 F (650-820 C). Above 1500 F (820 C), the effect of age hardening is lost and the alloy is used in the annealed condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: Ni-185. Producer or source: Carpenter Technology Corporation. Originally published February 1973, revised August 1989.
Journal Articles
Alloy Digest (1990) 39 (1): Fe-89.
Published: 01 January 1990
... PYROMET ALLOY CTX-909 exhibits a low and relatively constant thermal coefficient of expansion over a broad temperature range, high hot hardness and good thermal fatigue resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Abstract
View article
PDF
PYROMET ALLOY CTX-909 exhibits a low and relatively constant thermal coefficient of expansion over a broad temperature range, high hot hardness and good thermal fatigue resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-89. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1973) 22 (5): Ni-190.
Published: 01 May 1973
... PYROMET X-751 is an age hardenable nickel-base alloy with good stress-rupture properties at 1600 F. It is highly resistant to chemical corrosion and oxidation. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep...
Abstract
View article
PDF
PYROMET X-751 is an age hardenable nickel-base alloy with good stress-rupture properties at 1600 F. It is highly resistant to chemical corrosion and oxidation. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-190. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1973) 22 (6): Ni-192.
Published: 01 June 1973
... PYROMET 90 is a precipitation-hardenable nickel-base alloy with high strength at high temperatures. It is highly resistant to oxidation, scaling, heat and corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep...
Abstract
View article
PDF
PYROMET 90 is a precipitation-hardenable nickel-base alloy with high strength at high temperatures. It is highly resistant to oxidation, scaling, heat and corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-192. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1974) 23 (12): Ni-212.
Published: 01 December 1974
... PYROMET 625 is a nonmagnetic alloy with outstanding strength and toughness from cryogenic temperatures to 2000 F. It has excellent fatigue strength and stress-corrosion-cracking resistance to chloride ions. Some typical applications are heat shields, chemical plant hardware and special seawater...
Abstract
View article
PDF
PYROMET 625 is a nonmagnetic alloy with outstanding strength and toughness from cryogenic temperatures to 2000 F. It has excellent fatigue strength and stress-corrosion-cracking resistance to chloride ions. Some typical applications are heat shields, chemical plant hardware and special seawater applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-212. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1997) 46 (5): Fe-56.
Published: 01 May 1997
... AND ALLOYS CC@Q@ht1997,AShiASM~~A2~tS maandDataalwwnamlypical.nottoba uwdkn~~final~. Filing Code: Fe-56 m Iron Alloy izit I mm Revised May 1997 l uf&mdwASM IntamabaI MatadkPah.Ohio4#73-&W2 216-332-5151 f=ar216-336da MemscKvOpaAsM-lna..o PYROMET@ ALLOY CTX-1 (Controlled-Expansion Superalloy) Pyromet Cl-X-1...
Abstract
View article
PDF
Pyromet CTX-1 is a high-strength, precipitation-hardenable superalloy exhibiting a low coefficient of thermal expansion and high strength up to about 1200 deg F. The alloy possesses high hot hardness and good thermal fatigue resistance. Its applications include components for gas turbine engines, hot-work die applications and high-pressure hydrogen environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: FE-56. Producer or source: Carpenter. Originally published February 1976, revised May 1997.
Journal Articles
Alloy Digest (1989) 38 (10): Ni-189.
Published: 01 October 1989
... PYROMET Alloy 80A, a high-temperature nickel-base alloy is characterized by its excellent creep resistance, high fatigue properties under very arduous conditions and high oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well...
Abstract
View article
PDF
PYROMET Alloy 80A, a high-temperature nickel-base alloy is characterized by its excellent creep resistance, high fatigue properties under very arduous conditions and high oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and machining. Filing Code: Ni-189. Producer or source: Carpenter Technology Corporation. Originally published April 1973, revised October 1989.
Journal Articles
Alloy Digest (1991) 40 (12): Ni-397.
Published: 01 December 1991
... PYROMET alloy M-252 was designed for use in highly stressed parts operating at temperatures up to 1600 F (871 C). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature...
Abstract
View article
PDF
PYROMET alloy M-252 was designed for use in highly stressed parts operating at temperatures up to 1600 F (871 C). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and machining. Filing Code: Ni-397. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1973) 22 (12): Ni-198.
Published: 01 December 1973
... PYROMET 102 is a nonmagnetic, nickel-chromium base alloy which is solid solution strengthened by the refractory metals niobium, tungsten and molybdenum. It possesses excellent corrosion properties, strength, ductility, toughness and structural stability. It is used as tubing and piping for steam...
Abstract
View article
PDF
PYROMET 102 is a nonmagnetic, nickel-chromium base alloy which is solid solution strengthened by the refractory metals niobium, tungsten and molybdenum. It possesses excellent corrosion properties, strength, ductility, toughness and structural stability. It is used as tubing and piping for steam and gas turbines, rocket engines, heat shields, furnace hardware, chemical plant hardware and in sea water environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-198. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1991) 40 (10): Ni-237.
Published: 01 October 1991
... PYROMET alloy 41, a precipitation hardening nickel-base alloy possesses high strength in the 1200/1800 F (649/986 C) temperature range This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information...
Abstract
View article
PDF
PYROMET alloy 41, a precipitation hardening nickel-base alloy possesses high strength in the 1200/1800 F (649/986 C) temperature range This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-237. Producer or source: Carpenter Technology Corporation. Originally published December 1976, revised October 1991.
Journal Articles
Alloy Digest (1964) 13 (10): TS-152.
Published: 01 October 1964
... Pyromet 882 is an air-hardening 5% chromium tool steel recommended for high temperature applications up to 1000 F. It has extremely high tensile and creep strength. It is used for such critical applications as structural components in aircraft and missiles which require either extremely high...
Abstract
View article
PDF
Pyromet 882 is an air-hardening 5% chromium tool steel recommended for high temperature applications up to 1000 F. It has extremely high tensile and creep strength. It is used for such critical applications as structural components in aircraft and missiles which require either extremely high strength (over 260,000 psi) at ambient temperature or high creep and rupture strength at temperatures of about 800 to 1200 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-152. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1992) 41 (6): SS-530.
Published: 01 June 1992
... SANDVIK SANICRO 31HT is an austenitic iron-nickel-chromium alloy characterized by very good resistance to oxidation with good mechanical properties at elevated temperatures. It is recommended for resistance element sheathing, pyrometer tubes, airheaters, equipment for heat treating, furnace tubes...
Abstract
View article
PDF
SANDVIK SANICRO 31HT is an austenitic iron-nickel-chromium alloy characterized by very good resistance to oxidation with good mechanical properties at elevated temperatures. It is recommended for resistance element sheathing, pyrometer tubes, airheaters, equipment for heat treating, furnace tubes, and other equipment in the petrochemical industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-530. Producer or source: Sandvik.
Journal Articles
Alloy Digest (1971) 20 (9): SS-259.
Published: 01 September 1971
... 52000 1200 28000 1350 11800 1500 6500 1700 4300 1800 2000 1900 1500 2000 1100 65000 44000 40000 37000 34000 22000 Elongation (2 in.) % 29 20 20 20 ;: 99 97 0.269 7.45 0.11 5.9 x 10-6 6.3 x 10-6 6.4 x 10-6 7.0 x 10-6 7.5 x 10-6 8.0 x 10-6 105-l 15 107-l 16 114-120 12&123 DOI: 10.31399/asm.ad.ss0259...
Abstract
View article
PDF
Armco 18 SR is a ferritic stainless steel that provides excellent resistance to high temperature scaling. It is readily welded by conventional methods and is not subject to troublesome embrittlement or loss of corrosion resistance in the heat-affected zones that affect many other straight chromium alloys. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-259. Producer or source: Armco Steel Corporation, Advanced Materials Division.
Journal Articles
Alloy Digest (1969) 18 (1): TS-213.
Published: 01 January 1969
..., psi Thermal coef. expansion/OF 80400oF so-SOOOF SO-145OoF SOO-14500F PROPERTIES As-quenched 56-58 600 50-52 1000 48-50 1050 47-49 1100 4648 1150 4446 1200 42-44 1250 4042 1300 3840 Table 1 - TYPICAL HARDNESS DATA (I x I bars, oil quenched from 16700F & tempered) Tempering Rockwell Brinell Temrrure...
Abstract
View article
PDF
HEPPENSTALL C58 is an alloy tool and die steel furnished in the prehardened and in the annealed conditions. It is used for dies where very high compressive strength and resistance to softening at elevated temperatures are required. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-213. Producer or source: Midvale-Heppenstall Company.
Journal Articles
Alloy Digest (1955) 4 (2): SS-25.
Published: 01 February 1955
.../cc 23.00-30.00 Density, Ib./cu.in. 1.00 max. Specific electrical resistance, microhms/cm3 1.00 max. Melting range, OF. 0.03 max. Structure 0.04 max. Magnetic permeability, annealed balance Specific heat, Cal/X/g (0-100°C) Thermal conductivity, caI/cm2/sec/ C/cm at 100°C. at 500°C. Thermal coef...
Abstract
View article
PDF
ENDURO HC is a high chromium heat and corrosion resisting steel of the AISI Type 446 grade. It is magnetic and cannot be hardened materially by heat treatment. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-25. Producer or source: Republic Steel Corporation.
Journal Articles
Alloy Digest (1963) 12 (9): Ni-86.
Published: 01 September 1963
.../cu.in. Melting point, OF (apptoa.) Thermal coef. expansion/OC x 10s6 20-100°C 20-500% loo-2oo"c 400-5OOOC Electrical resistiviry, microhms-cm PROPERTIES Table 1 - TYPICAL MECHANICAL PROPERTIES - Bar Hot-Rolled Annealed Tensile strength, psi 121600 105700 Yield strength, psi (0.2%) 77300 46200 Elongation...
Abstract
View article
PDF
Corronel 230 is a nickel-chromium alloy having high resistance to corrosion by hot nitric acid and excellent resistance to attack at elevated temperatures from oxidizing and reducing atmospheres high in sulfur. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-86. Producer or source: Henry Wiggin & Company Ltd.