Alloy Digest (1966) 15 (9): Ni-117.
Published: 01 September 1966
... Pyromet 860 is a high temperature alloy with an unusual combination of strength and ductility in the 1350 F range. It is a precipitation hardening alloy recommended for turbine parts and other high temperature applications. This datasheet provides information on composition, physical properties...