Alloy Digest (1970) 19 (12): SS-247.
Published: 01 December 1970
... PYROMET 538 is a solid-solution strengthened, austenitic alloy with a desirable combination of strength, corrosion resistance, oxidation resistance, and economy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep...
Journal Articles
Alloy Digest (1977) 26 (6): SS-340.
Published: 01 June 1977
... PYROMET A-286 is an age-hardenable austenitic iron-nickel-chromium alloy designed for service up to 1300 F (704 C) on jobs requiring high strength and good corrosion resistance at the operating temperature. It offers high ductility in notched sections. Pyromet A-286 is used in jet engines...
Journal Articles
Alloy Digest (2012) 61 (3): Ni-695.
Published: 01 March 2012
... Pyromet Alloy 617 is both oxidation resistant and very strong at high temperatures. It has one of the highest allowable stress values in the ASME Boiler and Pressure Vessel Code at 982 deg C (1800 deg F). This datasheet provides information on composition, physical properties, elasticity, tensile...
Journal Articles
Alloy Digest (1986) 35 (9): SS-474.
Published: 01 September 1986
... PYROMET V-57 is an austenitic, iron-base precipitation-hardening alloy designed for service up to 1400 F (760 C) with good corrosion resistance at operating temperatures. The alloy is usually consumable-electrode, vacuum melted. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1987) 36 (7): Fe-78.
Published: 01 July 1987
...) Heat Treatment B lOOO(538) 110000(758) *ICI = 2, low-stress ground specimens. Properties are lowered if lathe- turned specimens are used. 210 2000 Heat Treatment: The optimum heat treatment for Pyromet CTX-3 varies with property requirements: Heat Treatment A: Warm-worked material is solution treated...
Journal Articles
Alloy Digest (1998) 47 (2): Ni-536.
Published: 01 February 1998
... Pyromet 31V is a sulfidation resistant, precipitation hardenable superalloy with unusual combination of corrosion resistance and strength to 816 C (1500 F). It has excellent resistance to hot sulfidation attack and has been used in truck and locomotive diesel valve service. This datasheet provides...
Journal Articles
Alloy Digest (1977) 26 (12): Ni-252.
Published: 01 December 1977
... PYROMET 31 is a nickel-base superalloy that exhibits an unusual combination of corrosion resistance and strength to temperatures as high as 1500 F (816 C). It has excellent resistance to hot sulfidation attack such as could occur in truck and locomotive diesel valve service. This datasheet...
Journal Articles
Alloy Digest (1997) 46 (5): Fe-56.
Published: 01 May 1997
... Pyromet CTX-1 is a high-strength, precipitation-hardenable superalloy exhibiting a low coefficient of thermal expansion and high strength up to about 1200 deg F. The alloy possesses high hot hardness and good thermal fatigue resistance. Its applications include components for gas turbine engines...
Journal Articles
Alloy Digest (1986) 35 (6): Fe-72.
Published: 01 June 1986
... PYROMET N-155 has inherent high-temperature properties and is recommended for high-stress service up to 1500 F or for moderate-stress service up to 2000 F. It has good ductility, can be readily fabricated and machined and its high-temperature oxidation resistance is excellent. This datasheet...
Journal Articles
Alloy Digest (1991) 40 (12): Ni-397.
Published: 01 December 1991
... PYROMET alloy M-252 was designed for use in highly stressed parts operating at temperatures up to 1600 F (871 C). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature...
Journal Articles
Alloy Digest (1989) 38 (10): Ni-189.
Published: 01 October 1989
... PYROMET Alloy 80A, a high-temperature nickel-base alloy is characterized by its excellent creep resistance, high fatigue properties under very arduous conditions and high oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well...
Journal Articles
Alloy Digest (1973) 22 (7): Ni-193.
Published: 01 July 1973
... PYROMET 718 is an alloy designed to display exceptionally high yeild, tensile and stress-rupture properties at temperatures up to 1300 F. (704 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1973) 22 (6): Ni-192.
Published: 01 June 1973
... PYROMET 90 is a precipitation-hardenable nickel-base alloy with high strength at high temperatures. It is highly resistant to oxidation, scaling, heat and corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep...
Journal Articles
Alloy Digest (1978) 27 (3): Ni-187.
Published: 01 March 1978
... PYROMET 680 is a nonmagnetic nickel-base alloy that derives its exceptional properties up to 2200 F (1200 C) from solid solution strengthening. Among its applications are gas turbine components and furnace hardware. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2015) 64 (9): Ni-723.
Published: 01 September 2015
... Pyromet alloy 706 has similarities to alloy 718, but improves fabricability and welding. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming...
Journal Articles
Alloy Digest (2021) 70 (11): Ni-777.
Published: 01 November 2021
... CarTech 617 (Pyromet 617) is a corrosion and oxidation-resistant, high-temperature nickel-chromium-cobalt-molybdenum alloy. It is solid-solution strengthened with cobalt and molybdenum. Oxidation resistance is imparted through the addition of chromium and aluminum. This datasheet provides...
Journal Articles
Alloy Digest (1991) 40 (10): Ni-237.
Published: 01 October 1991
... PYROMET alloy 41, a precipitation hardening nickel-base alloy possesses high strength in the 1200/1800 F (649/986 C) temperature range This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information...
Journal Articles
Alloy Digest (1999) 48 (10): SS-765.
Published: 01 October 1999
... nickel alloy that is precipitation hardened and has good strength and corrosion resistance to 760 °C (1400 °F). It is commonly used for engine valve applications. NCF 3015 alloy is both manufactured and sold under license from Hitachi. Pyromet is a registered trademark of Carpenter Technology Corpo...
Journal Articles
Alloy Digest (1994) 43 (2): Fe-105.
Published: 01 February 1994
... hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, high tensile and rupture strengths, and good thermal fatigue resistance. This alloy offers a significant improvement in environmental resistance over Pyromet alloys CTX-1, CTX-3, and CTX-909 due...