Alloy Digest (1970) 19 (2): Cu-211.
Published: 01 February 1970
... PROMET 2S is a highly leaded bronze recommended for bearings under boundary or mixed film conditions. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength. It also includes information on corrosion resistance as well...