Alloy Digest (2010) 59 (6): SA-617.
Published: 01 June 2010
... PremoMet offers superior strength, toughness and fatigue resistance and may be considered as a lower-cost alternative to many cobalt containing steel alloys. Consider PremoMet alloy for high-demand power train components in heavy-duty diesel engines and other commercial ground transportation...