1-20 of 719 Search Results for

Pitting corrosion

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1993) 42 (10): SS-552.
Published: 01 October 1993
... AVESTA 654 SMO is an austenitic stainless steel which due to its high content of molybdenum and nitrogen possesses excellent resistance to pitting and crevice corrosion. It also has very high resistance to general corrosion in acids, especially those containing halide ions. Furthermore, its...
Journal Articles
Alloy Digest (1992) 41 (7): Ni-407.
Published: 01 July 1992
... and crevice corrosion in severely Table 5 - Resistance to pitting in solution saturated with sodium chloride and sulfur dioxide at 176┬░F (8O Cr 1 MaximumDcpthofAuackc Weld Metal mils mm Base Metal mils mm 7.1 0.18 5.5 0.14 13.0 0.33 Specimen Type Alloy 622 sheet, GTA welded tiFillerMetal622...
Journal Articles
Alloy Digest (1992) 41 (10): Ni-414.
Published: 01 October 1992
... WIDE METALS AND ALLOYS ~hl1992AlbyD@~t.kAUfi@~r- PdWmdby: AI&y DQW. Inc 1201677.9161 ~eog$gyJ 27 Canlii Slme~. Orange, N.J. 07050 I U.S.& INCONEL FILLER METAL 622 (Pitting and Crevice Corrosion Resistant Nickel-base Filler Metal) lNCONEL* FILLER METAL 622 is a highly alloyed product used for joining...
Journal Articles
Alloy Digest (1998) 47 (6): Cu-617.
Published: 01 June 1998
... Monel Electrode 187 is an all-position copper-nickel welding electrode that meets all the requirements of applicable U.S. military specifications. The all-position electrode is of major importance in boatyards and desalination plants in resistance to pitting corrosion and avoidance of the danger...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-600.
Published: 01 January 2003
... Allcorr (UNS N06110) is a single-phase, non-age-hardenable, nickel-base alloy for service in highly corrosive environments. It is characterized by outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress-corrosion cracking. The alloy...
Journal Articles
Alloy Digest (1983) 32 (2): Ni-283.
Published: 01 February 1983
... NICROFER 4221 is a fully austenitic nickel-chromium-iron-molybdenum-copper alloy that is stabilized (against intergranular corrosion) by an addition of titanium. It is resistant to stress-corrosion cracking, pitting corrosion and oxidizing and non-oxidizing hot acids. It has good mechanical...
Journal Articles
Alloy Digest (1982) 31 (11): SS-415.
Published: 01 November 1982
... CRONIFER 2205 LCN is a low-carbon nitrogen-alloyed stainless steel with a ferritic-austenitic duplex structure. It has excellent resistance to stress-corrosion cracking in solutions containing chloride ions. Its resistance to pitting corrosion is good; both base metal and welded material...
Journal Articles
Alloy Digest (1977) 26 (1): SS-336.
Published: 01 January 1977
... UHB Stainless 34L is noted for its extra-low carbon content (0.03% max) and high molybdenum content (4.3%). It has excellent resistance to uniform corrosion and to pitting corrosion. Its tensile strength is approximately the same as that of other austenitic stainless steels. This steel...
Journal Articles
Alloy Digest (1983) 32 (2): SS-420.
Published: 01 February 1983
... EASTERN STAINLESS Type 316 is a chromium-nickel-molybdenum steel. The molybdenum (2-3%) gives it the greatest resistance to pitting corrosion of any of the AISI standard grades of austenitic stainless steel. This extra measure of corrosion resistance makes this grade particularly suitable for uses...
Journal Articles
Alloy Digest (2000) 49 (5): SS-787.
Published: 01 May 2000
... Nirosta 4429 is a low-carbon, high-nitrogen version of type 316 stainless steel. The low carbon imparts intergranular corrosion resistance while the nitrogen imparts both higher strength and some increased pitting corrosion resistance. It is recommended for use as welded parts that need...
Journal Articles
Alloy Digest (2013) 62 (12): SS-1164.
Published: 01 December 2013
... MAGIVAL MG3 is a ferritic free machining stainless steel grade with similar magnetic properties to MG1 (Alloy Digest SS-1159, October 2013); it has better pitting corrosion resistance due to its molybdenum content, allowing applications in mild chloride corrosive environments. Magival is a group...
Journal Articles
Alloy Digest (2002) 51 (1): SS-839.
Published: 01 January 2002
.... The enhanced addition of molybdenum renders this steel particularly suitable for use in environments that have a high pitting corrosion risk. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature...
Journal Articles
Alloy Digest (1996) 45 (12): SS-664.
Published: 01 December 1996
... Remanit 4401 is a chromium-nickel-molybdenum austenitic stainless steel. The molybdenum (2 to 2.5%) gives it resistance to pitting corrosion, more than most of the standard grades of austenitic stainless steels. This extra measure of corrosion resistance makes this grade particularly suitable...
Journal Articles
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
... Inconel alloy 22 is an advanced corrosion-resistant alloy with exceptional resistance to aqueous and pitting corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2022) 71 (11): Cu-935.
Published: 01 November 2022
.... It has excellent deep drawing characteristics and resistance to pitting corrosion when exposed to severe weather and water environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (2023) 72 (9): Ni-786.
Published: 01 September 2023
... VDM 33 (Nicrofer 3033) is an austenitic alloy that has an excellent resistance against common corrosion and pitting corrosion in media containing chloride due to its well-balanced analysis and extraordinarily high chromium content. Also because of its very high strength and good workability, VDM...
Journal Articles
Alloy Digest (1994) 43 (9): Ni-465.
Published: 01 September 1994
... Nicrofer 6616hMo is an austenitic low-carbon nickel-molybdenum-chromium alloy characterized by very good resistance to corrosive media under highly oxidizing conditions and by excellent resistance to crevice and pitting corrosion. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1993) 42 (4): SS-542.
Published: 01 April 1993
... TYPE 317L, 317LX, and 317LXN are austenitic alloys with varying molybdenum and nitrogen contents and thus have varying levels of resistance to pitting corrosion. All are low carbon to resist sensitization. All three alloys are intended for severe service conditions such as flue gas desulfurization...
Journal Articles
Alloy Digest (2001) 50 (5): SS-822.
Published: 01 May 2001
... ALZ 316HMo is an austenitic stainless steel with good formability, corrosion resistance, toughness, and mechanical properties. This grade is molybdenum rich, making it particularly suitable for use in environments that have a high risk or pitting corrosion. This datasheet provides information...
Journal Articles
Alloy Digest (2013) 62 (3): SS-1139.
Published: 01 March 2013
... ATI 436S is a ferritic stainless steel stabilized with titanium. It is superior to ATI Type 409 and 430 in general and pitting corrosion resistance. The ATI 436S alloy exhibits machining, welding, and forming characteristics similar to those of other stabilized, ferritic stainless steels...