Skip Nav Destination
Close Modal
Search Results for
PYROTOOL M
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-3 of 3 Search Results for
PYROTOOL M
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1971) 20 (1): Ni-160.
Published: 01 January 1971
... PYROTOOL M is an austenitic precipitation-hardenable nickel-base alloy designed for highly stressed parts operating at temperatures up to 1500 F (816 C). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Abstract
View article
PDF
PYROTOOL M is an austenitic precipitation-hardenable nickel-base alloy designed for highly stressed parts operating at temperatures up to 1500 F (816 C). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-160. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1972) 21 (1): Ni-167.
Published: 01 January 1972
... PYROTOOL 7 has been designed to display high tensile and yield properties with good hardness at temperatures up to 1300 F. It is used for high-temperature tooling, extrusion dies, forging dies, rams, mandrels, holders, rings, dummy blocks, liners, etc. This datasheet provides information...
Abstract
View article
PDF
PYROTOOL 7 has been designed to display high tensile and yield properties with good hardness at temperatures up to 1300 F. It is used for high-temperature tooling, extrusion dies, forging dies, rams, mandrels, holders, rings, dummy blocks, liners, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-167. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1972) 21 (4): SS-271.
Published: 01 April 1972
.... Because of its ductility, Pyrotool 15 can also be machined in the aged condition at a hardness of Rockwell C50. In the solution-treated condition, this material machines at 60-80 surface feet per minute (IS-24 m/min) using tool material of T-15. With tungsten carbide use surface feet per minute of 120-140...
Abstract
View article
PDF
PYROTOOL 15 is a low-carbon martensitic precipitation-hardenable (maraging) heat-resistant steel designed to possess high strength from room temperature to 1050 F. Uses include tooling applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-271. Producer or source: Carpenter.