1-6 of 6 Search Results for

PYROMET 88

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1989) 38 (8): Ni-185.
Published: 01 August 1989
... PYROMET alloy 88 is an age hardenable nickel-base alloy with high strength good corrosion and oxidation resistance. It possesses low creep rate in the temperature range 1200-1500 F (650-820 C). Above 1500 F (820 C), the effect of age hardening is lost and the alloy is used in the annealed...
Journal Articles
Alloy Digest (2012) 61 (3): Ni-695.
Published: 01 March 2012
... (34) 610 (88) 64 649 (1200) 250 (36) 587 (85) 60 760 (1400) 272 (39) 534 (77) 52 871 (1600) 269 (39) 358 (52) 43 982 (1800) 125 (18) 173 (25) 69 Heat Treatment: Pyromet Alloy 617 has two basic heat treatments: 1. High solution anneal 1121 to 1177 ºC (2050 to 2150 ºF), air quench or faster. 2...
Journal Articles
Alloy Digest (2015) 64 (9): Ni-723.
Published: 01 September 2015
... Pyromet alloy 706 has similarities to alloy 718, but improves fabricability and welding. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming...
Journal Articles
Alloy Digest (1978) 27 (3): Ni-187.
Published: 01 March 1978
... PYROMET 680 is a nonmagnetic nickel-base alloy that derives its exceptional properties up to 2200 F (1200 C) from solid solution strengthening. Among its applications are gas turbine components and furnace hardware. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1953) 2 (3): SS-6.
Published: 01 March 1953
... 1800 IOGO (Recommended design stress - 30% of limiting creep stress) 45000 26000 15000 88 5 170 14 90 25 7 :: Table 4 STRESS-l-O-RUPTURE (Aged Castings) Temperature StfCSS F Hours psi 1600 10 11400 1600 100 8700 1600 1000 6000 1800 10 5800 1800 100 4300 1800 1000 2800 Table 6 TEMPERATURE RESISTANCE OF...
Journal Articles
Alloy Digest (1974) 23 (1): Cu-274.
Published: 01 January 1974
... 700F Tensile strength, psi 90000 60000 Yield point. psi 54000 20000 Elongation (2 in 96 ;: 49 Reduction of area, % 77 Irod impact, ft-lb 88 80 Table 6 - EMF OF Cu-Ni 55-45 ALLOY VERSUS PLATINUM (Cold junction at 320F) (See General Characertistics) Temperature Emf Temperature Emf OF mv OF mv -300 -200...