Alloy Digest (2018) 67 (2): SS-1279.
Published: 01 February 2018
... Pyrodur 4910 is a high-temperature resistant, chromium, nickel, molybdenum, nitrogen, and boron containing austenitic stainless steel. It has superior high-temperature strength and oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties...