1-2 of 2 Search Results for

PROJECT 70 TYPE 316/316L

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2003) 52 (3): SS-878.
Published: 01 March 2003
... Carpenter Project 70+ Type 316/316L is a modified version of Type 316/316L stainless steel with improved machinability when compared to conventional 316/316L. The alloys are non-hardenable austenitic chromium-nickel-molybdenum steels and are good general-purpose products for simple and complex...
Journal Articles
Alloy Digest (2002) 51 (1): SS-841.
Published: 01 January 2002
... thermal Density Specific heat conductivity expansion Btu/ Btu/ Alloy kg/m3 lb/in.3 J/kg K lb °F W/m K (ft h °F) 10 6/K 10 6/°F 304, 304L 7940 0.287 500 0.119 16.3 9.42 16.6 9.22 316, 316L 8030 0.290 450 0.107 16.2 9.36 16.5 9.17 19D 7770 0.281 471 0.112 15.9 9.19 14.4 8.00 2205 7850 0.284 470...