Alloy Digest (1993) 42 (11): SS-553.
Published: 01 November 1993
... PRODEC STAINLESS TYPE 304L is a standardized grade in plate and bar with an improved machining capability over the conventional AISI Type 304L. It is a product of extensive laboratory testing and application proven. Its improved machinability offers: shorter machining time; longer tool life...