Skip Nav Destination
Close Modal
Search Results for
POLMAX
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
POLMAX
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2005) 54 (2): SS-918.
Published: 01 February 2005
... Polmax was developed to be both highly polishable and corrosion resistant for extreme surface finishes such as in lens molds. Polmax has excellent polishability, good corrosion resistance, good wear resistance, good machinability, and good stability in hardening. It is used for applications where...
Abstract
View article
PDF
Polmax was developed to be both highly polishable and corrosion resistant for extreme surface finishes such as in lens molds. Polmax has excellent polishability, good corrosion resistance, good wear resistance, good machinability, and good stability in hardening. It is used for applications where extreme surface finishes are required, such as lens molds, molds for compact discs and memory discs, and molds for med-ical applications. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties. It also includes information on corrosion resistance and surface qualities as well as heat treating and surface treatment. Filing Code: SS-918. Producer or source: Böhler-Uddeholm North America.