Journal Articles
Alloy Digest (2015) 64 (9): SA-730.
Published: 01 September 2015
... PERFORM 460 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 460 in the title refers to the minimum yield strength in MPa (67 ksi). The USA equivalent is Perform 67. This datasheet provides information on composition, tensile...
Journal Articles
Alloy Digest (1985) 34 (7): SS-460.
Published: 01 July 1985
... and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-460. Producer or source: Avesta Stainless Inc.. Producer or Source: Avesta Stainless Inc. Copyright © ASM International® 1996...
Journal Articles
Alloy Digest (2011) 60 (3): SA-621.
Published: 01 March 2011
... (to be indicated on the order) Dillinal 460/630 N 20 ( 4) 45 (33) Dillinal 460/630 NL 40 ( 40) 45 (33) Heat Treatment: If stress-relieving treatment is necessary, this is usually performed on the finished welded vessel. The stress-relieving treatment should be performed at temperatures between 530 to 560 ºC (985...
Journal Articles
Alloy Digest (2017) 66 (2): SA-778.
Published: 01 February 2017
... to the specimen width (produc t thickness). No impact test is performed on products below 5 mm (0.2 in.) in thickness. If special agreement is made for carrying out a bend test, it will be carried out on transverse specimens, the mandrel diameter being a minimum of four times the material thickness and a bending...
Journal Articles
Alloy Digest (2007) 56 (6): Cu-748.
Published: 01 June 2007
... Olin alloy C19720 is a dispersion-strengthened high-conductivity alloy for automotive power distribution. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. and bend strength. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (2019) 68 (1): SA-835.
Published: 01 January 2019
... to allow degassing. Suitable parameters must be calculated for the laser according to the wall thickness, type of weld, finish, and materials being joined. The heat-affected zone displays moderate hardening, which is generally noncritical. General Characteristics Owing to their good processing performance...
Journal Articles
Alloy Digest (1991) 40 (5): P-26.
Published: 01 May 1991
... composites and adhe- sives. It offers superior hot/wet performance characteris- tics. TACTIX 556 can be cured with a variety of con- ventional hardeners to optimize specific properties. Diaminodiphenylsulfone (DDS) appears to give the best balance of glass transition temperature and moisture properties when...
Journal Articles
Alloy Digest (2000) 49 (9): TS-580.
Published: 01 September 2000
... Boehler K340 ISODUR has a balanced composition for cold work forming operations like stamping and cutting. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on high temperature performance as well as heat treating...
Journal Articles
Alloy Digest (2015) 64 (9): SA-731.
Published: 01 September 2015
.../asm.ad.sa0731 structure and/or the expected stress condition after welding requires a reduction of the residual stresses. Stress relieving of Histar steel grades is performed at temperatures between 530 °C and 580 °C (986 and 1076 °F). The holding time should be two minutes per mm (0.04 in.) of product...
Journal Articles
Alloy Digest (2011) 60 (6): SS-1094.
Published: 01 June 2011
... psi) 200 (29.0) Shear modulus, GPa (106 psi) 77 (11.17) Poisson s ratio 0.32 See Tables 1, 2, and 3 for room temperature, elevated temperature and representative creep properties. Fatigue. Fatigue data for unwelded 3CR12 is shown in Fig. 1. The data described here refer to tests performed under...
Journal Articles
Alloy Digest (2020) 69 (1): SS-1314.
Published: 01 January 2020
...) 10.1 (5.6) 10.1 (5.6) 0 538 °C (32 1000 °F) 12.0 (6.6) 11.9 (6.6) Specific heat capacity J/(kg K) (cal/(g °C)) 0 100 °C (32 212 °F) 460 (0.11) 460 (0.11) Source: AK Steel and ASM Handbook,Vol. 1: Properties and Selection: Irons, Steels, and High-Performance Alloys Type 435 Mod (UNS S44500) 7690 (0.28...
Journal Articles
Alloy Digest (1994) 43 (6): SA-476.
Published: 01 June 1994
... hardness for martensitic alloy steels. This behavior is confirmed for the HARDWEAR F steels. Other abrasion-resistant plate steels perform simi- larly in the laboratory test, which measures the weight loss of the test pm in milligrams. The primary ordering requirements for the Hardwear steels is minimum...
Journal Articles
Alloy Digest (1987) 36 (10): Fe-80.
Published: 01 October 1987
... (68-752) 20-450 (68-842) 20-500 (68-932) Total Expansion 0.68 x IO 1.1I I.55 I .98 2.44 2.88 3.34 3.84 4.37 OF EXPANSION Mean Linear Coefficient of Expansion 8.5 x IO- 8.5 8.6 8.6 Yi.7 8.7 8.8 8.9 9. I Heat Treatment: Annealing can be performed in the range 850-1000 C ( I562-1832OF). It should...
Journal Articles
Alloy Digest (2016) 65 (5): SA-751.
Published: 01 May 2016
... toughness and creep. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: SA-751. Producer or source: Böhler Edelstahl GmbH & Company KG. Producer or Source: Böhler Edelstahl GmbH & Company KG Copyright © ASM International®...
Journal Articles
Alloy Digest (2011) 60 (8): SA-630.
Published: 01 August 2011
... for the selection of the material. Forming Properties. Diros 500 can be hot or cold formed. Cold forming can be performed at room temperature or between 50 and DOI: 10.31399/asm.ad.sa0630 100 ºC (122 and 212 ºF) below the tempering temperature. For both cases it must be generally taken into account that the plates...
Journal Articles
Alloy Digest (2015) 64 (12): SA-735.
Published: 01 December 2015
... and their uses. Stress Relieving. A stress relief post-weld heat treatment (PWHT) may be necessary when the layout of the structure and/or the expected stress condition after welding requires a reduction of the residual stresses. Stress relieving of Fritenar steel grades is performed at temperatures between 530...
Journal Articles
Alloy Digest (2017) 66 (1): Cu-856.
Published: 01 January 2017
... Alloy KHP 102 (UNS C19010) is a high performance copper alloy with additions for strength while maintaining high conductivity. KHP 102 belongs to the group of CuNiSi alloys and is particularly suitable for use in electrical and electronic products. This datasheet provides information...
Journal Articles
Alloy Digest (2007) 56 (2): SS-987.
Published: 01 February 2007
... the producer. Fig. 1 Tempering chart. Hardening: holding time 30 min in oil; tempering 2 × 2 h; specimen size 20 × 20 mm square DOI: 10.31399/asm.ad.ss0987 Corrosion Resistance: The corrosion-resistant surface area after performance of the salt- spray test (DIN 50021) on hardened and tempered steels is shown...
Journal Articles
Alloy Digest (2000) 49 (5): TS-577.
Published: 01 May 2000
... treatment to al- low for dimensional changes or distortion that may occur. For reference, the size change should not exceed 0.0015 in./in. per side (0.003 in. overall) if stress relieving has been performed following rough machining. BOHLER M310 ISOPLAST® Filing Code TS-577 Tool Steel May 2000 Table 1...
Journal Articles
Alloy Digest (2006) 55 (5): SS-963.
Published: 01 May 2006
... the alloy. This hardening treatment also tempers the martensitic structure, increasing ductility and toughness. Solution annealing should be performed in air, argon, or dry hydrogen. Cracked ammonia and endothermic atmospheres are likely to contaminate the metal. Remove machining oils and forming lubricants...