Alloy Digest (2015) 64 (8): SA-729.
Published: 01 August 2015
... PERFORM 420 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 420 in the title refers to the minimum yield strength in MPa (61 ksi). The USA equivalent is Perform 60. This datasheet provides information on composition, tensile...
Journal Articles
Alloy Digest (1985) 34 (6): CS-107.
Published: 01 June 1985
... in machining. especially when computer-controlled equipment is being used. Predictable Performance: Today. machine shops demand predictability because of the need for accuracy in analyzing and estimating part production. The uniformity of Series 83-420 steel bars helps to make the machining...
Journal Articles
Alloy Digest (2020) 69 (7): SS-1321.
Published: 01 July 2020
... CarTech 420 is a hardenable, 13% chromium, martensitic stainless steel with higher strength and hardness, and better wear resistance than Type 410 stainless steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2001) 50 (7): SS-826.
Published: 01 July 2001
... TLS 420 MQ os a mold-quality stainless steel that meets requirements in polishability, corrosion resistance, and wear resistance by special melting and forging practices. Is is used in plastic mold cavities and surgical instruments. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2015) 64 (6): SS-1212.
Published: 01 June 2015
... relieved condition in order to maximize its corrosion resistance. In the as-annealed condition, this grade will result in poor corrosion performance and is not recommended. Specification Equivalents: UNS S42000 ASTM A176 AMS 5506 AK 420 STAINLESS STEEL (Martensitic Stainless Steel) Filing Code: SS-1212...
Journal Articles
Alloy Digest (2009) 58 (1): TS-676.
Published: 01 January 2009
... Micro-Melt 420-CW is a powder-produced wear-resistant tool steel with corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on corrosion and wear resistance as well as...
Journal Articles
Alloy Digest (1975) 24 (7): SS-314.
Published: 01 July 1975
... CRUCIBLE CSM 420 is furnished in the annealed condition designed primarily for use in the molding of all plastics, including the vinyl-base and other corrosive plastics. Crucible's exclusive Densified process is used in the manufacture of this steel to insure freedom porosity, pinholes or voids...
Journal Articles
Alloy Digest (1976) 25 (8): SS-331.
Published: 01 August 1976
... WIDE METALS AND ALLOYS Publisbd by Engineering Alloys Digest, Inc. UHB STAVAX* ESR Upper Montclair. New Jersey (Stainless Plastic-Mold Steel; AISI Type 420) UHB STAVAX ESR is a high-chromium (13.6%) martensitic stainless plastic-mold steel. It is Electra-Slag Refined (ESR) to provide the best...
Journal Articles
Alloy Digest (2000) 49 (8): SS-801.
Published: 01 August 2000
... Allegheny Ludlum Type 420 is a hardenable, straight-chromium stainless steel with wear and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (2018) 67 (12): sa-831.
Published: 01 December 2018
... MHZ 420 (mininum yield strength of 420 MPa) is one of a series of microalloyed cold forming steels. The high-strength properties result from precipitation hardening thanks to finely-dispersed carbonitrides and a fine-grained microstructure. Even very small amounts of the elements titanium and/or...
Journal Articles
Alloy Digest (2010) 59 (9): Cu-787.
Published: 01 September 2010
.... AMPCOLOY® 88 (High-Performance Copper Alloy) AMPCOLOY® 88 Chemical Composition, wt (Nominal) Cobalt + Nickel 3 Beryllium 0.5 Others 0.5 max Copper bal Physical Properties: Density, g/cm3 (lb/in.3) 8.75 (0.315) Coefficient of thermal expansion, 10 6 /K (10 6/ºF) 17 (9.44) Electrical conductivity, 106S/m...
Journal Articles
Alloy Digest (2010) 59 (10): Cu-789.
Published: 01 October 2010
... MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Copper October 2010 Cu-789 Ampcoloy 95 has slightly higher mechanical properties than most alloys in its class. Applications include spot welding electrodes. AMPCOLOY® 95 (Extruded High-Performance Copper Alloy) AMPCOLOY...
Journal Articles
Alloy Digest (1998) 47 (2): SS-707.
Published: 01 February 1998
..., nitro- gen, and oxygen contents. This process provides steel with the optimum combination of cleanliness, refined structure, strength, and isotropic properties, which makes it the ideal material for high performance dies and molds. Finkl42OM Premium Quality exhibits improved toughness over AISI 420...
Journal Articles
Alloy Digest (1983) 32 (2): SS-420.
Published: 01 February 1983
..., elasticity, tensile properties, and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-420. Producer or source: Eastern Stainless Steel...
Journal Articles
Alloy Digest (2013) 62 (7): SA-679.
Published: 01 July 2013
... Armox 440T combines good ballistic properties with excellent toughness. Hardness is 420-480 HBW. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: SA-679...
Journal Articles
Alloy Digest (2008) 57 (5): SS-1012.
Published: 01 May 2008
... Uginox MA2 (X20Cr13, No. 1.4021; AISI type 420) is an age-hardenable martensitic stainless steel, mostly used where a sharp edge for cutting is needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1993) 42 (1): Ni-420.
Published: 01 January 1993
... Code: Ni-420. Producer or source: Cannon-Muskegon Corporation. Producer or Source: Cannon-Muskegon Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition CMSX-3 corrosion-resistant alloys creep properties physical properties Filing Code: Ni-420...
Journal Articles
Alloy Digest (1981) 30 (7): Cu-420.
Published: 01 July 1981
... provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-420. Producer or source: Ampco Metal Inc.. Producer or Source: Ampco...
Journal Articles
Alloy Digest (2014) 63 (11): SS-1188.
Published: 01 November 2014
... Carpenter CTS 20HC is a version of type 420 martensitic stainless steel containing nominal 0.5% carbon content. The chemical composition and processing of CTS 20HC have been tailored to provide a uniform, fine carbide structure that can be considered for the manufacture of thin sections and fine...
Journal Articles
Alloy Digest (2008) 57 (7): SS-1015.
Published: 01 July 2008
... Uginox MA3 (X30Cr13, No. 1.4028; AISI 420) is an age-hardenable martensitic stainless steel, mostly used where a sharp edge for cutting is needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on...