Skip Nav Destination
Close Modal
Search Results for
Ovahyd 600
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
Ovahyd 600
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (7): SA-548.
Published: 01 July 2005
... The Ovahyd 600, 650, 700 family of steels encompasses a range of strength levels. The steels have a guaranteed yield strength matching the name. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming, machining, and joining...
Abstract
View article
PDF
The Ovahyd 600, 650, 700 family of steels encompasses a range of strength levels. The steels have a guaranteed yield strength matching the name. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming, machining, and joining. Filing Code: SA-548. Producer or source: Ovako Steel Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (6): SA-544.
Published: 01 June 2005
... Ovahyd 450 is a steel developed for highly stressed cylinder and piston rod applications in the hydraulic industry. The yield strength (MPa) corresponds to the alloy name. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming...
Abstract
View article
PDF
Ovahyd 450 is a steel developed for highly stressed cylinder and piston rod applications in the hydraulic industry. The yield strength (MPa) corresponds to the alloy name. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming, machining, and joining. Filing Code: SA-544. Producer or source: Ovako Steel Inc.