Alloy Digest (2020) 69 (11): SS-1329.
Published: 01 November 2020
... Outokumpu Moda 410S/4000 is a 13% Cr, ferritic stainless steel that is used in applications requiring good resistance to mildly corrosive environments. It is a low carbon, non-hardening modification of Type 410 stainless steel. This datasheet provides information on composition, physical...