Alloy Digest (2007) 56 (8): TS-653.
Published: 01 August 2007
... Orvar Superior is a premium Cr-Mo-V alloyed hot-work die steel with good resistance to thermal fatigue. The name “superior” is used to indicate that close control in special melting and refining has attained a high purity and very fine structure that produces isotropic properties. This datasheet...