Publisher: Journals Gateway
Alloy Digest (1997) 46 (10): SA-488.
Published: 01 October 1997
... and joining. Filing Code: SA-488. Producer or source: Oregon Steel Mills. Producer or Source: Oregon Steel Mills Copyright ┬ę ASM International┬« 1997 1997 ASM International bridges chemical composition heat treatability joinability Oregon formalloy ASTM 514 tensile properties DATA ON WORLD...