Alloy Digest (1956) 5 (9): TS-50.
Published: 01 September 1956
... OLYMPIC FM is a high-carbon high-chromium steel with greatly improved machinability due to carefully controlled sulphide additives. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-50. Producer...