Alloy Digest (2000) 49 (1): Cu-645.
Published: 01 January 2000
... Olin C688 is a brass enriched with both aluminum and cobalt for added strength and stress relaxation resistance. The alloy is ideal for springs. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes...
Journal Articles
Alloy Digest (2000) 49 (2): Cu-647.
Published: 01 February 2000
... Olin C654 is a 95.4Cu-3.0Si-1.5Sn-0.1Cr bronze alloy with high strength, good formability, and stress-relaxation resistance. Uses include springs and connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...