Alloy Digest (2020) 69 (2): Cu-905.
Published: 01 February 2020
... Olin Brass Alloy C19020 is a copper-nickel-tin low-alloyed copper. It was developed as alloy NB-105 by Dowa Metaltech Company Limited, Japan, to meet increasing requirements of current carrying capacity, stiffness, formability and service temperature survivability being demanded by the automotive...
Journal Articles
Alloy Digest (2004) 53 (11): Cu-727.
Published: 01 November 2004
... or source: Olin Brass. Producer or Source: Olin Brass Copyright Ā© ASM InternationalĀ® 2004 2004 ASM International chemical composition elasticity Olin alloy C19020 physical properties tensile properties thermal properties UNS C19020 Chemical Composition, wt Tin 0.30 0.9 Nickel...