Alloy Digest (2016) 65 (4): SA-748.
Published: 01 April 2016
... Ovako 42CrMo4 is a quench and tempered steel with high strength and good toughness. The Cromax family consists of hard chrome-plated long product in the form of bars and tubes. These products are available in different steel grades with executions in a broad range of sizes. (See also Ovako 42CrMo4...