Alloy Digest (2016) 65 (1): SS-1235.
Published: 01 January 2016
...-1235. Producer or source: Outokumpu Stainless Bar. Producer or Source: Outokumpu Stainless Bar Copyright Ā© ASM InternationalĀ® 2016 2016 ASM International chemical composition elasticity formability heat treatability joinability OUTOKUMPU Supra 316LN Plus physical properties...