... OUTOKUMPU MODA 430/4016 is a 16% chromium ferritic stainless steel that combines good mechanical properties with good corrosion resistance and heat and oxidation resistance up to 815 °C (1500 °F). It is the most commonly used ferritic stainless steel grade and can be used to replace type 304...
Journal Articles
Alloy Digest (2021) 70 (11): SS-1341.
Published: 01 November 2021
... Outokumpu Moda 439/4510 is a titanium-stabilized 17% chromium ferritic stainless steel that exhibits improved corrosion resistance, formability, and weldability when compared to Outokumpu Moda 430/4016. It is best suited for mildly corrosive environments. Because of its titanium alloying...