Alloy Digest (2018) 67 (2): SS-1278.
Published: 01 February 2018
... Copyright ┬ę ASM International┬« 2018 2018 ASM International corrosion-resistant alloys elasticity hardness joinability OUTOKUMPU FORTA H500 physical properties tensile properties workability thermal properties Forta H500 is an austenitic stainless steel in which manganese replaces some...