Alloy Digest (1981) 30 (10): Sn-11.
Published: 01 October 1981
... OSTALLOY 281-338 is a non-eutectic alloy with a melting range of 281-338 F (138-170 C). It provides scientists, engineers, manufacturers and technicians with an easily castable material that is ready for use soon after it freezes. It has the advantage that it can be recovered easily and used again...