... OSTALLOY 281-338 is a non-eutectic alloy with a melting range of 281-338 F (138-170 C). It provides scientists, engineers, manufacturers and technicians with an easily castable material that is ready for use soon after it freezes. It has the advantage that it can be recovered easily and used again...
Journal Articles
Alloy Digest (1980) 29 (5): Bi-17.
Published: 01 May 1980
... OSTALLOY 281 is a bismuth-base eutectic alloy. Its melting temperature is 281 F (138 C); this is the highest melting point of the bismuth-base alloys commonly used in industry. It provides an easily castable material ready for use soon after it freezes. The alloy can be recovered easily...