Alloy Digest (1980) 29 (11): Bi-20.
Published: 01 November 1980
... OSTALLOY 158 is a bismuth-base, eutectic alloy that melts at 158 F (70 C). It provides engineers and technicians with an easily castable material that is ready for use as soon as it freezes. It can be recovered easily and recycled into new uses any number of times. Its many uses include holding...