Alloy Digest (1982) 31 (3): Bi-28.
Published: 01 March 1982
... OSTALLOY 136 is a bismuth-base, low-melting eutectic alloy; it melts at 136 F (57.8 C), hence its identifying number. This alloy finds wide use in industry and in laboratories because of its low melting temperature and controlled-shrinkage characteristics. It can be recovered easily and recycled...