Alloy Digest (2004) 53 (6): Cu-715.
Published: 01 June 2004
... Olin Alloy C5218 is a phosphor bronze alloy given both dispersion- and solid-solution strengthening for applications in the automotive connector market. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. Filing Code: CU-715...