Alloy Digest (2007) 56 (6): Cu-748.
Published: 01 June 2007
... Olin alloy C19720 is a dispersion-strengthened high-conductivity alloy for automotive power distribution. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. and bend strength. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (2020) 69 (2): Cu-905.
Published: 01 February 2020
... conductivity or strength requirements, alloys C19720 or C18080 should be considered. Supplier Olin Brass GBC Metals, LLC 4801 Olympia Park Plaza, Suite 3500 Louisville, Kentucky 40241 USA Tel: +1 502 873 3000 Web: www.olinbrass.com ISSN: 002-614X Cu-905B ...