Alloy Digest (1963) 12 (3): Al-123.
Published: 01 March 1963
... NORAL 162 is an age-hardenable aluminum casting alloy. It has low thermal expansion, good high temperature strength and bearing (frictional) properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear...